Dielectric, ferroelectric and induced strain behavior of PLZT 9/65/35 ceramics modified by Bi<inf>2</inf>O<inf>3</inf> and CuO co-doping

© 2016 Elsevier Ltd and Techna Group S.r.l. PLZT 9/65/35 (Pb 0.91 La 0.09 (Zr 0.65 Ti 0.35 ) 0.9775 O 3 ) ceramics with addition of 0.25, 0.5 and 1.0 wt% of Bi 2 O 3 /CuO (where the ratio of Bi 2 O 3 :CuO=9:1 by mole) were prepared by sintering at the temperatures between 1000 and 1200 °C. It was fo...

Full description

Saved in:
Bibliographic Details
Main Authors: Somwan S., Ngamjarurojana A., Limpichaipanit A.
Format: Journal
Published: 2017
Online Access:https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84961879954&origin=inward
http://cmuir.cmu.ac.th/jspui/handle/6653943832/41752
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Chiang Mai University