Dielectric and mechanical properties of mullite/modified batio<inf>3</inf> composites

© 2016 Trans Tech Publications, Switzerland. Composites between mullite and modified BT were prepared by a conventional technique. The samples were calcined at 1300 °C for 2 h. The composites were sintered at 1250 °C for 2 h. The dielectric and mechanical properties samples were investigated. The me...

Full description

Saved in:
Bibliographic Details
Main Authors: Lertcumfu N., Sanjoom K., Arkornsakul P., Sweatman D., Phatungthane T., Chokethawai K., Rujijanagul G.
Format: Book Series
Published: 2017
Online Access:https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84958191341&origin=inward
http://cmuir.cmu.ac.th/jspui/handle/6653943832/42329
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Chiang Mai University
Description
Summary:© 2016 Trans Tech Publications, Switzerland. Composites between mullite and modified BT were prepared by a conventional technique. The samples were calcined at 1300 °C for 2 h. The composites were sintered at 1250 °C for 2 h. The dielectric and mechanical properties samples were investigated. The mechanical properties were found to improve after sintering at a suitable temperature. Addition of the BT produced an improvement in dielectric constant due to the BT has high piezoelectric properties. A higher dielectric constant for a sample contained higher amount of the BT was related with a higher polarization in the samples.