Relaxor behaviour of K <inf>0.5</inf>Bi <inf>0.5</inf>NbO <inf>3</inf>- BiScO <inf>3</inf> ceramics
Dielectric properties of (1 - x)K 0.5 Bi 0.5 TiO 3 - xBiScO 3 ceramics have been studied for compositions x < 0.5. Single-phase solid solutions occurred for compositions x < 0.25. A frequency-dependent dielectric relaxation was observed, consistent with relaxor behaviour. This gave r...
Saved in:
Main Authors: | Kruea-In C., Rujijanagul G., Zhu F., Milne S. |
---|---|
Format: | Journal |
Published: |
2017
|
Online Access: | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84861813860&origin=inward http://cmuir.cmu.ac.th/jspui/handle/6653943832/42841 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Chiang Mai University |
Similar Items
-
Relaxor behaviour of K<inf>0.5</inf>Bi<inf>0.5</inf>NbO<inf>3</inf>- BiScO<inf>3</inf>ceramics
by: Chatchai Kruea-In, et al.
Published: (2018) -
Properties of 0.94Bi<inf>0.5</inf>Na<inf>0.5</inf>TiO<inf>3</inf>-0. 06BiAlO<inf>3</inf>ceramics prepared by two steps sintering technique
by: Supalak Manotham, et al.
Published: (2018) -
Properties of 0.94Bi<inf>0.5</inf>Na<inf>0.5</inf>TiO<inf>3</inf>-0. 06BiAlO<inf>3</inf>ceramics prepared by two steps sintering technique
by: Supalak Manotham, et al.
Published: (2018) -
Phase transition and tolerance factor relationship of lead-free (Bi<inf>0.5</inf>K<inf>0.5</inf>)TiO<inf>3</inf>-Bi(Mg<inf>0.5</inf>Ti<inf>0.5</inf>)O<inf>3</inf> piezoelectric ceramics
by: Jaita P., et al.
Published: (2017) -
Phase transition and tolerance factor relationship of lead-free (Bi<inf>0.5</inf>K<inf>0.5</inf>)TiO<inf>3</inf>-Bi(Mg<inf>0.5</inf>Ti<inf>0.5</inf>)O<inf>3</inf>piezoelectric ceramics
by: Pharatree Jaita, et al.
Published: (2018)