Effect of temperature on loss mechanism of 0.7PMN-0.3PZT ceramics

© 2015 Elsevier B.V. In this work, 0.7Pb(Mg 1/3 Nb 2/3 )O 3 -0.3Pb(Zr 0.52 Ti 0.48 )O 3 (0.7PMN-0.3PZT) relaxor ferroelectric ceramic was prepared. The dielectric constant was measured by LCR meter at frequencies of 1-100 kHz to observe ferroelectric-paraelectric phase transition T m . To investigat...