Piezoelectric and ferroelectric properties of lead-free Bi<inf>0.5</inf>(Na<inf>0.80</inf>K<inf>0.20</inf>)<inf>0.5</inf>TiO<inf>3</inf>-(Ba<inf>0.98</inf>Nd<inf>0.20</inf>)TiO<inf>3</inf>binary system
© 2017 Taylor & Francis Group, LLC. This research was conducted to investigate the effect of (Ba 0.98 Nd 0.20 )TiO 3 addition on properties of Bi 0.5 (Na 0.80 K 0.20 ) 0.5 TiO 3 ceramic. The binary system having composition of(1-x)Bi 0.5 (Na 0.80 K 0.20 ) 0.5 TiO 3 -x(Ba 0.98 Nd 0.20 )TiO 3 or...
Saved in:
Main Authors: | , , , |
---|---|
Format: | Journal |
Published: |
2018
|
Subjects: | |
Online Access: | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85015851613&origin=inward http://cmuir.cmu.ac.th/jspui/handle/6653943832/46867 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Chiang Mai University |
id |
th-cmuir.6653943832-46867 |
---|---|
record_format |
dspace |
spelling |
th-cmuir.6653943832-468672018-04-25T07:28:47Z Piezoelectric and ferroelectric properties of lead-free Bi<inf>0.5</inf>(Na<inf>0.80</inf>K<inf>0.20</inf>)<inf>0.5</inf>TiO<inf>3</inf>-(Ba<inf>0.98</inf>Nd<inf>0.20</inf>)TiO<inf>3</inf>binary system Pimpilai Wannasut Pharatree Jaita Sukanda Jiansirisomboon Anucha Watcharapasorn Materials Science Agricultural and Biological Sciences © 2017 Taylor & Francis Group, LLC. This research was conducted to investigate the effect of (Ba 0.98 Nd 0.20 )TiO 3 addition on properties of Bi 0.5 (Na 0.80 K 0.20 ) 0.5 TiO 3 ceramic. The binary system having composition of(1-x)Bi 0.5 (Na 0.80 K 0.20 ) 0.5 TiO 3 -x(Ba 0.98 Nd 0.20 )TiO 3 or (1-x)BNKT-xBNdT (x = 0, 0.01, 0.02, 0.03, 0.04, 0.05, 0.06 mol fraction) was prepared by a conventional mixed oxide and sintering method. From the characterization results, the ceramics sintered at 1125°C had relative density of more than 98% of their theoretical values regardless of BNdT content. X-ray diffraction pattern of the ceramics showed a single perovskite structure with mixed rhombohedral and tetragonal phases (i.e. within MPB region). Scanning electron micrographs showed a cubic-like grain shape and the grain size decreased with increasing BNdT content. The ceramic with x = 0.04 showed relatively high room temperature dielectric constant with low loss (ϵ r = 1670, tanδ = 0.0532), high piezoelectric coefficient (d 33 = 192 pC/N) and good ferroelectric properties (P r = 19.12 µC/cm 2 , E c = 13.54 kV/cm and R sq = 1.52) which may be suitable for transducer and actuator applications. 2018-04-25T07:03:29Z 2018-04-25T07:03:29Z 2017-01-02 Journal 16078489 10584587 2-s2.0-85015851613 10.1080/10584587.2017.1284536 https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85015851613&origin=inward http://cmuir.cmu.ac.th/jspui/handle/6653943832/46867 |
institution |
Chiang Mai University |
building |
Chiang Mai University Library |
country |
Thailand |
collection |
CMU Intellectual Repository |
topic |
Materials Science Agricultural and Biological Sciences |
spellingShingle |
Materials Science Agricultural and Biological Sciences Pimpilai Wannasut Pharatree Jaita Sukanda Jiansirisomboon Anucha Watcharapasorn Piezoelectric and ferroelectric properties of lead-free Bi<inf>0.5</inf>(Na<inf>0.80</inf>K<inf>0.20</inf>)<inf>0.5</inf>TiO<inf>3</inf>-(Ba<inf>0.98</inf>Nd<inf>0.20</inf>)TiO<inf>3</inf>binary system |
description |
© 2017 Taylor & Francis Group, LLC. This research was conducted to investigate the effect of (Ba 0.98 Nd 0.20 )TiO 3 addition on properties of Bi 0.5 (Na 0.80 K 0.20 ) 0.5 TiO 3 ceramic. The binary system having composition of(1-x)Bi 0.5 (Na 0.80 K 0.20 ) 0.5 TiO 3 -x(Ba 0.98 Nd 0.20 )TiO 3 or (1-x)BNKT-xBNdT (x = 0, 0.01, 0.02, 0.03, 0.04, 0.05, 0.06 mol fraction) was prepared by a conventional mixed oxide and sintering method. From the characterization results, the ceramics sintered at 1125°C had relative density of more than 98% of their theoretical values regardless of BNdT content. X-ray diffraction pattern of the ceramics showed a single perovskite structure with mixed rhombohedral and tetragonal phases (i.e. within MPB region). Scanning electron micrographs showed a cubic-like grain shape and the grain size decreased with increasing BNdT content. The ceramic with x = 0.04 showed relatively high room temperature dielectric constant with low loss (ϵ r = 1670, tanδ = 0.0532), high piezoelectric coefficient (d 33 = 192 pC/N) and good ferroelectric properties (P r = 19.12 µC/cm 2 , E c = 13.54 kV/cm and R sq = 1.52) which may be suitable for transducer and actuator applications. |
format |
Journal |
author |
Pimpilai Wannasut Pharatree Jaita Sukanda Jiansirisomboon Anucha Watcharapasorn |
author_facet |
Pimpilai Wannasut Pharatree Jaita Sukanda Jiansirisomboon Anucha Watcharapasorn |
author_sort |
Pimpilai Wannasut |
title |
Piezoelectric and ferroelectric properties of lead-free Bi<inf>0.5</inf>(Na<inf>0.80</inf>K<inf>0.20</inf>)<inf>0.5</inf>TiO<inf>3</inf>-(Ba<inf>0.98</inf>Nd<inf>0.20</inf>)TiO<inf>3</inf>binary system |
title_short |
Piezoelectric and ferroelectric properties of lead-free Bi<inf>0.5</inf>(Na<inf>0.80</inf>K<inf>0.20</inf>)<inf>0.5</inf>TiO<inf>3</inf>-(Ba<inf>0.98</inf>Nd<inf>0.20</inf>)TiO<inf>3</inf>binary system |
title_full |
Piezoelectric and ferroelectric properties of lead-free Bi<inf>0.5</inf>(Na<inf>0.80</inf>K<inf>0.20</inf>)<inf>0.5</inf>TiO<inf>3</inf>-(Ba<inf>0.98</inf>Nd<inf>0.20</inf>)TiO<inf>3</inf>binary system |
title_fullStr |
Piezoelectric and ferroelectric properties of lead-free Bi<inf>0.5</inf>(Na<inf>0.80</inf>K<inf>0.20</inf>)<inf>0.5</inf>TiO<inf>3</inf>-(Ba<inf>0.98</inf>Nd<inf>0.20</inf>)TiO<inf>3</inf>binary system |
title_full_unstemmed |
Piezoelectric and ferroelectric properties of lead-free Bi<inf>0.5</inf>(Na<inf>0.80</inf>K<inf>0.20</inf>)<inf>0.5</inf>TiO<inf>3</inf>-(Ba<inf>0.98</inf>Nd<inf>0.20</inf>)TiO<inf>3</inf>binary system |
title_sort |
piezoelectric and ferroelectric properties of lead-free bi<inf>0.5</inf>(na<inf>0.80</inf>k<inf>0.20</inf>)<inf>0.5</inf>tio<inf>3</inf>-(ba<inf>0.98</inf>nd<inf>0.20</inf>)tio<inf>3</inf>binary system |
publishDate |
2018 |
url |
https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85015851613&origin=inward http://cmuir.cmu.ac.th/jspui/handle/6653943832/46867 |
_version_ |
1681422954221535232 |