Fabrication of glass foams from industrial wastes used as insulating board
Insulating glass foam (IGF) was successfully fabricated by wet process. The starting proportion of 65 wt% waste glass, 12 wt% slag, 23 wt% commercial soap was added with 15 wt% Na 2 SiO 3 and represented then was sintered at 725 °C. The IGF had cellular structure with the macro-pore size at 0.428 m...