Surface modification of the Ti-Al alloys at 1000-1200 K

Alloys of Ti-40wt.%Al, Ti-43wt.%Al, Ti-48wt.%Al, Ti-47wt. %Al-2wt.%Nb-2wt.%Cr and Ti-47wt.%Al-2wt.%Nb-2wt.%Mn-0.8wt.%TiB2 were nitrided in ammonia at atmospheric pressure and at 1000-1200 K for 3.6×105 s. The hardness and thickness of the nitride layers on the alloys were measured. It was found that...