Preparation and characterization of BiVO<inf>4</inf>powder by the sol-gel method
Bismuth vanadate (BiVO 4 ) powder was successfully prepared by the sol-gel method. Bismuth nitrate and ammonium vanadate were used as the starting precursors with mole ratio of 1:1 in ethanol media at 70°C for 1 h. The yellow gel was calcined at 400-600°C for 2 h. The phase of BiVO 4 powder was char...