Morphology development of ZnO produced by sonothermal process
Wurtzite ZnO (hcp) was produced by the 80 °C sonothermal reactions of 1:5, 1:10, and 1:20 molar ratios of Zn(NO3)2· 6H2O:NaOH in water, containing 2 g, 5 g, 10 g, and 20 g of polyethylene glycol (PEG) with the molecular weights (MWs) of 6000, 10000, and 20000 for 1 h, 3 h, and 5 h. ZnO phase with di...
Saved in:
Main Authors: | Siriprapha Jattukul, Somchai Thongtem, Titipun Thongtem |
---|---|
Format: | Journal |
Published: |
2018
|
Subjects: | |
Online Access: | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=79957500055&origin=inward http://cmuir.cmu.ac.th/jspui/handle/6653943832/49788 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Chiang Mai University |
Similar Items
-
Morphology development of ZnO produced by sonothermal process
by: Jattukul S., et al.
Published: (2014) -
The effect of H2O and PEG on the morphologies of ZnO nanostructures synthesized under microwave radiation
by: Titipun Thongtem, et al.
Published: (2018) -
Characterization of nanostructured ZnO produced by microwave irradiation
by: Titipun Thongtem, et al.
Published: (2018) -
Effect of basicity on the morphologies of ZnO produced using a sonochemical method
by: Titipun Thongtem, et al.
Published: (2018) -
Effect of basicity on the morphologies of ZnO produced using a sonochemical method
by: Titipun Thongtem, et al.
Published: (2018)