Fabrication of ferroelectric bismuth titanate glass-ceramic by incorporation method

In this work the fabrication of glass-ceramics containing ferroelectric BIT crystals was carried out by incorporation method. The BIT powder was prepared by conventional ceramic method with calcination temperature of 800°C. In order to prepare bismuth titanate glass ceramic by incorporation method,...

Full description

Saved in:
Bibliographic Details
Main Author: Pengpat K.
Format: Conference or Workshop Item
Language:English
Published: 2014
Online Access:http://www.scopus.com/inward/record.url?eid=2-s2.0-62949221878&partnerID=40&md5=4d172e08312069efb7e4bb264006e85d
http://cmuir.cmu.ac.th/handle/6653943832/5385
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Chiang Mai University
Language: English
id th-cmuir.6653943832-5385
record_format dspace
spelling th-cmuir.6653943832-53852014-08-30T02:56:28Z Fabrication of ferroelectric bismuth titanate glass-ceramic by incorporation method Pengpat K. In this work the fabrication of glass-ceramics containing ferroelectric BIT crystals was carried out by incorporation method. The BIT powder was prepared by conventional ceramic method with calcination temperature of 800°C. In order to prepare bismuth titanate glass ceramic by incorporation method, the BIT powder was mixed with 25-95 mol% B2O3 as a glass former. The batches were melted in an air atmosphere using an electric furnace, at 1150°C for 15 minutes. After that, the melts were quenched between the stainless steel plates at room temperature. It was found that crystallization of unexpected Bi2Ti4O11 phase occurred in most of the glass - ceramics with the amount of B2O3 less than 70 mol%. This may cause from the evaporation of Bi2O3 during melting. Besides, glass could only be obtained from the melt of 80 mol% B 2O3 batch. In this glass, however, the small amount of TiC2 crystals was detected using SEM technique. The glasses with the amount of B2O3 more than 80% shows severe phase separation and crystallization of TiO2 and B2O3. The glasses of 80 mol% B2O3 composition were subjected to heat - treatment processes at 300 to 500°C. It was found that the crystallization of Bi2Ti4O11 phase occurred at 500°C while at 300°C and 400°C the glasses were still amorphous. The maximum dielectric constant (εr) of the heat treated glass ceramics was found in the range of 22-30. © 2008 Trans Tech Publications, Switzerland. 2014-08-30T02:56:28Z 2014-08-30T02:56:28Z 2008 Conference Paper 9780878493562 10226680 75596 http://www.scopus.com/inward/record.url?eid=2-s2.0-62949221878&partnerID=40&md5=4d172e08312069efb7e4bb264006e85d http://cmuir.cmu.ac.th/handle/6653943832/5385 English
institution Chiang Mai University
building Chiang Mai University Library
country Thailand
collection CMU Intellectual Repository
language English
description In this work the fabrication of glass-ceramics containing ferroelectric BIT crystals was carried out by incorporation method. The BIT powder was prepared by conventional ceramic method with calcination temperature of 800°C. In order to prepare bismuth titanate glass ceramic by incorporation method, the BIT powder was mixed with 25-95 mol% B2O3 as a glass former. The batches were melted in an air atmosphere using an electric furnace, at 1150°C for 15 minutes. After that, the melts were quenched between the stainless steel plates at room temperature. It was found that crystallization of unexpected Bi2Ti4O11 phase occurred in most of the glass - ceramics with the amount of B2O3 less than 70 mol%. This may cause from the evaporation of Bi2O3 during melting. Besides, glass could only be obtained from the melt of 80 mol% B 2O3 batch. In this glass, however, the small amount of TiC2 crystals was detected using SEM technique. The glasses with the amount of B2O3 more than 80% shows severe phase separation and crystallization of TiO2 and B2O3. The glasses of 80 mol% B2O3 composition were subjected to heat - treatment processes at 300 to 500°C. It was found that the crystallization of Bi2Ti4O11 phase occurred at 500°C while at 300°C and 400°C the glasses were still amorphous. The maximum dielectric constant (εr) of the heat treated glass ceramics was found in the range of 22-30. © 2008 Trans Tech Publications, Switzerland.
format Conference or Workshop Item
author Pengpat K.
spellingShingle Pengpat K.
Fabrication of ferroelectric bismuth titanate glass-ceramic by incorporation method
author_facet Pengpat K.
author_sort Pengpat K.
title Fabrication of ferroelectric bismuth titanate glass-ceramic by incorporation method
title_short Fabrication of ferroelectric bismuth titanate glass-ceramic by incorporation method
title_full Fabrication of ferroelectric bismuth titanate glass-ceramic by incorporation method
title_fullStr Fabrication of ferroelectric bismuth titanate glass-ceramic by incorporation method
title_full_unstemmed Fabrication of ferroelectric bismuth titanate glass-ceramic by incorporation method
title_sort fabrication of ferroelectric bismuth titanate glass-ceramic by incorporation method
publishDate 2014
url http://www.scopus.com/inward/record.url?eid=2-s2.0-62949221878&partnerID=40&md5=4d172e08312069efb7e4bb264006e85d
http://cmuir.cmu.ac.th/handle/6653943832/5385
_version_ 1681420415565561856