Effects of heat treatment on hardness and dry wear properties of a semi-solid processed Fe-27 wt pct Cr-2.9 wt pct C cast iron
Effects of heat treatments on hardness and dry wear properties of a semi-solid processed Fe-26.96 wt pct Cr-2.91 wt pct C cast iron were studied. Heat treatments included tempering at 500°C, destabilisation at 1075°C and destabilisation at 1075°C plus tempering at 500°C, all followed by air cooling....