Influence of mixed solvents on characteristics and photoluminescence of GdVO<inf>4</inf>: Eu<sup>3+</sup>nanophosphors synthesized by solvothermal method

© 2016 by American Scientific Publishers. GdVO4:Eu3+nanoparticles were synthesized by a solvothermal method at 200°C for 24 h, followed by calcination at 600°C for 3 h. The effects of mixed solvents (water:methanol, water:ethanol, water:ethylene glycol and water:glycerol) on purity, crystallinity, s...

Full description

Saved in:
Bibliographic Details
Main Authors: Watcharapong Pudkon, Sila Kittiwachana, Titipun Thongtem, Somchai Thongtem, Sulawan Kaowphong
Format: Journal
Published: 2018
Subjects:
Online Access:https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84964768852&origin=inward
http://cmuir.cmu.ac.th/jspui/handle/6653943832/55927
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Chiang Mai University
id th-cmuir.6653943832-55927
record_format dspace
spelling th-cmuir.6653943832-559272018-09-05T03:05:09Z Influence of mixed solvents on characteristics and photoluminescence of GdVO<inf>4</inf>: Eu<sup>3+</sup>nanophosphors synthesized by solvothermal method Watcharapong Pudkon Sila Kittiwachana Titipun Thongtem Somchai Thongtem Sulawan Kaowphong Materials Science © 2016 by American Scientific Publishers. GdVO4:Eu3+nanoparticles were synthesized by a solvothermal method at 200°C for 24 h, followed by calcination at 600°C for 3 h. The effects of mixed solvents (water:methanol, water:ethanol, water:ethylene glycol and water:glycerol) on purity, crystallinity, size and agglomeration behavior of the GdVO4:Eu3+nanoparticles were investigated. The products, characterized by powder X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR) and energy dispersive X-ray spectroscopy (EDS), were indexed as pure GdVO4with tetragonal structure. Field emission scanning electron microscope (FESEM) and transmission electron microscope (TEM) images revealed that the synthesized powders composed of spherical nanoparticles with diameters of about 15-40 nm. The difference in the characteristics of the synthesized nanoparticles could be related to the properties of the solvents used in the present work. The GdVO4:Eu3+nanoparticles synthesized using the mixed solvent of water:glycerol was smaller in size with soft agglomerations offering the highest photoluminescence (PL) emission intensity. Whereas, the PL intensity of the nanoparticles synthesized using water:ethylene glycol was lower than those of the others probably due to the existence of some defects in the crystals. 2018-09-05T03:05:09Z 2018-09-05T03:05:09Z 2016-01-01 Journal 19472943 19472935 2-s2.0-84964768852 10.1166/sam.2016.2617 https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84964768852&origin=inward http://cmuir.cmu.ac.th/jspui/handle/6653943832/55927
institution Chiang Mai University
building Chiang Mai University Library
country Thailand
collection CMU Intellectual Repository
topic Materials Science
spellingShingle Materials Science
Watcharapong Pudkon
Sila Kittiwachana
Titipun Thongtem
Somchai Thongtem
Sulawan Kaowphong
Influence of mixed solvents on characteristics and photoluminescence of GdVO<inf>4</inf>: Eu<sup>3+</sup>nanophosphors synthesized by solvothermal method
description © 2016 by American Scientific Publishers. GdVO4:Eu3+nanoparticles were synthesized by a solvothermal method at 200°C for 24 h, followed by calcination at 600°C for 3 h. The effects of mixed solvents (water:methanol, water:ethanol, water:ethylene glycol and water:glycerol) on purity, crystallinity, size and agglomeration behavior of the GdVO4:Eu3+nanoparticles were investigated. The products, characterized by powder X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR) and energy dispersive X-ray spectroscopy (EDS), were indexed as pure GdVO4with tetragonal structure. Field emission scanning electron microscope (FESEM) and transmission electron microscope (TEM) images revealed that the synthesized powders composed of spherical nanoparticles with diameters of about 15-40 nm. The difference in the characteristics of the synthesized nanoparticles could be related to the properties of the solvents used in the present work. The GdVO4:Eu3+nanoparticles synthesized using the mixed solvent of water:glycerol was smaller in size with soft agglomerations offering the highest photoluminescence (PL) emission intensity. Whereas, the PL intensity of the nanoparticles synthesized using water:ethylene glycol was lower than those of the others probably due to the existence of some defects in the crystals.
format Journal
author Watcharapong Pudkon
Sila Kittiwachana
Titipun Thongtem
Somchai Thongtem
Sulawan Kaowphong
author_facet Watcharapong Pudkon
Sila Kittiwachana
Titipun Thongtem
Somchai Thongtem
Sulawan Kaowphong
author_sort Watcharapong Pudkon
title Influence of mixed solvents on characteristics and photoluminescence of GdVO<inf>4</inf>: Eu<sup>3+</sup>nanophosphors synthesized by solvothermal method
title_short Influence of mixed solvents on characteristics and photoluminescence of GdVO<inf>4</inf>: Eu<sup>3+</sup>nanophosphors synthesized by solvothermal method
title_full Influence of mixed solvents on characteristics and photoluminescence of GdVO<inf>4</inf>: Eu<sup>3+</sup>nanophosphors synthesized by solvothermal method
title_fullStr Influence of mixed solvents on characteristics and photoluminescence of GdVO<inf>4</inf>: Eu<sup>3+</sup>nanophosphors synthesized by solvothermal method
title_full_unstemmed Influence of mixed solvents on characteristics and photoluminescence of GdVO<inf>4</inf>: Eu<sup>3+</sup>nanophosphors synthesized by solvothermal method
title_sort influence of mixed solvents on characteristics and photoluminescence of gdvo<inf>4</inf>: eu<sup>3+</sup>nanophosphors synthesized by solvothermal method
publishDate 2018
url https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84964768852&origin=inward
http://cmuir.cmu.ac.th/jspui/handle/6653943832/55927
_version_ 1681424596717273088