Microscopy and strength of borosilicate glass-to-Kovar alloy joints

The microstructural basis of the strength of borosilicate glass-to-Kovar alloy joints has been investigated where the alloy was preoxidised at 750 °C for 10 min in air. X-ray diffraction revealed that the oxide scale consisted of hematite and magnetite. Glass was bonded to the alloy by melting at 10...