Characterization of lead-free bismuth titanate (Bi4Ti 3O12) synthesized by a modified oxalate co-precipitation method
Bismuth titanate (Bi4Ti3O12) powders and ceramics were synthesized by a modified oxalate co-precipitation method, from the starting precursors of bismuth nitrate pentahydrate and titanium (IV) isoproproxide in the mole ratio of Bi: Ti of 4 : 3. The mill-precipitated powder was calcined at 500-800 °C...
Saved in:
Main Authors: | , |
---|---|
Format: | Article |
Language: | English |
Published: |
2014
|
Online Access: | http://www.scopus.com/inward/record.url?eid=2-s2.0-70350145181&partnerID=40&md5=6172c079a9683b5677cd9172a1dc55a3 http://cmuir.cmu.ac.th/handle/6653943832/5789 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Chiang Mai University |
Language: | English |
id |
th-cmuir.6653943832-5789 |
---|---|
record_format |
dspace |
spelling |
th-cmuir.6653943832-57892014-08-30T03:23:28Z Characterization of lead-free bismuth titanate (Bi4Ti 3O12) synthesized by a modified oxalate co-precipitation method Pookmanee P. Phanichphant S. Bismuth titanate (Bi4Ti3O12) powders and ceramics were synthesized by a modified oxalate co-precipitation method, from the starting precursors of bismuth nitrate pentahydrate and titanium (IV) isoproproxide in the mole ratio of Bi: Ti of 4 : 3. The mill-precipitated powder was calcined at 500-800 °C for 2 h. The phase transition was studied by an X-ray diffractometer. An orthorhombic structure was obtained after calcination at 700 °C for 2 h. The morphology was characterized by a scanning electron microscope. The average particle size increased as the calcination temperature increased. Powder calcined at 700 °C for 2 h was pressed into pellets. The pellets were sintered at 900 and 1000 °C for 2 h. The phase and microstructure of the ceramic in the pellets were investigated by an X-ray diffractometer and a scanning electron microscope. A single phase orthorhombic structure of bismuth titanate was obtained. The average particle size increased as the sintering temperature increased. The chemical composition of the ceramics was analyzed by an energy dispersive X-ray spectrometer (EDXS). The elemental composition of bismuth, titanium and oxygen showed the characteristic X-ray energy values. 2014-08-30T03:23:28Z 2014-08-30T03:23:28Z 2009 Article 12299162 http://www.scopus.com/inward/record.url?eid=2-s2.0-70350145181&partnerID=40&md5=6172c079a9683b5677cd9172a1dc55a3 http://cmuir.cmu.ac.th/handle/6653943832/5789 English |
institution |
Chiang Mai University |
building |
Chiang Mai University Library |
country |
Thailand |
collection |
CMU Intellectual Repository |
language |
English |
description |
Bismuth titanate (Bi4Ti3O12) powders and ceramics were synthesized by a modified oxalate co-precipitation method, from the starting precursors of bismuth nitrate pentahydrate and titanium (IV) isoproproxide in the mole ratio of Bi: Ti of 4 : 3. The mill-precipitated powder was calcined at 500-800 °C for 2 h. The phase transition was studied by an X-ray diffractometer. An orthorhombic structure was obtained after calcination at 700 °C for 2 h. The morphology was characterized by a scanning electron microscope. The average particle size increased as the calcination temperature increased. Powder calcined at 700 °C for 2 h was pressed into pellets. The pellets were sintered at 900 and 1000 °C for 2 h. The phase and microstructure of the ceramic in the pellets were investigated by an X-ray diffractometer and a scanning electron microscope. A single phase orthorhombic structure of bismuth titanate was obtained. The average particle size increased as the sintering temperature increased. The chemical composition of the ceramics was analyzed by an energy dispersive X-ray spectrometer (EDXS). The elemental composition of bismuth, titanium and oxygen showed the characteristic X-ray energy values. |
format |
Article |
author |
Pookmanee P. Phanichphant S. |
spellingShingle |
Pookmanee P. Phanichphant S. Characterization of lead-free bismuth titanate (Bi4Ti 3O12) synthesized by a modified oxalate co-precipitation method |
author_facet |
Pookmanee P. Phanichphant S. |
author_sort |
Pookmanee P. |
title |
Characterization of lead-free bismuth titanate (Bi4Ti 3O12) synthesized by a modified oxalate co-precipitation method |
title_short |
Characterization of lead-free bismuth titanate (Bi4Ti 3O12) synthesized by a modified oxalate co-precipitation method |
title_full |
Characterization of lead-free bismuth titanate (Bi4Ti 3O12) synthesized by a modified oxalate co-precipitation method |
title_fullStr |
Characterization of lead-free bismuth titanate (Bi4Ti 3O12) synthesized by a modified oxalate co-precipitation method |
title_full_unstemmed |
Characterization of lead-free bismuth titanate (Bi4Ti 3O12) synthesized by a modified oxalate co-precipitation method |
title_sort |
characterization of lead-free bismuth titanate (bi4ti 3o12) synthesized by a modified oxalate co-precipitation method |
publishDate |
2014 |
url |
http://www.scopus.com/inward/record.url?eid=2-s2.0-70350145181&partnerID=40&md5=6172c079a9683b5677cd9172a1dc55a3 http://cmuir.cmu.ac.th/handle/6653943832/5789 |
_version_ |
1681420491950129152 |