Ethanol sensing properties of CuO nanowires prepared by an oxidation reaction

The ethanol sensing properties of CuO nanowires prepared by oxidation reaction of copper plate have been examined. The characterization of CuO nanowires by FE-SEM, EDS, and TEM revealed diameters of 100-400 nm and a monoclinic structure with a growth direction along 〈1 1 0〉 direction. The ethanol se...

Full description

Saved in:
Bibliographic Details
Main Authors: Phathaitep Raksa, Atcharawan Gardchareon, Torranin Chairuangsri, Pongsri Mangkorntong, Nikorn Mangkorntong, Supab Choopun
Format: Journal
Published: 2018
Subjects:
Online Access:https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=57749122161&origin=inward
http://cmuir.cmu.ac.th/jspui/handle/6653943832/59439
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Chiang Mai University
id th-cmuir.6653943832-59439
record_format dspace
spelling th-cmuir.6653943832-594392018-09-10T03:20:07Z Ethanol sensing properties of CuO nanowires prepared by an oxidation reaction Phathaitep Raksa Atcharawan Gardchareon Torranin Chairuangsri Pongsri Mangkorntong Nikorn Mangkorntong Supab Choopun Chemical Engineering Materials Science The ethanol sensing properties of CuO nanowires prepared by oxidation reaction of copper plate have been examined. The characterization of CuO nanowires by FE-SEM, EDS, and TEM revealed diameters of 100-400 nm and a monoclinic structure with a growth direction along 〈1 1 0〉 direction. The ethanol sensing characteristics of CuO nanowires were studied at ethanol concentrations of 100-1000 ppm and working temperatures of 200-280 °C. An increase of resistance was observed under an ethanol vapor atmosphere due to the p-type semi-conducting property of CuO. It was found that the sensitivity, the response and the recovery time depended on the working temperatures and also ethanol concentration. The sensor exhibited the optimum sensitivity of 1.5 to ethanol vapor concentration of 1000 ppm at the working temperature of 240 °C with a response and recovery time of 110 and 120 s, respectively. © 2008 Elsevier Ltd and Techna Group S.r.l. 2018-09-10T03:15:12Z 2018-09-10T03:15:12Z 2009-03-01 Journal 02728842 2-s2.0-57749122161 10.1016/j.ceramint.2008.01.028 https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=57749122161&origin=inward http://cmuir.cmu.ac.th/jspui/handle/6653943832/59439
institution Chiang Mai University
building Chiang Mai University Library
country Thailand
collection CMU Intellectual Repository
topic Chemical Engineering
Materials Science
spellingShingle Chemical Engineering
Materials Science
Phathaitep Raksa
Atcharawan Gardchareon
Torranin Chairuangsri
Pongsri Mangkorntong
Nikorn Mangkorntong
Supab Choopun
Ethanol sensing properties of CuO nanowires prepared by an oxidation reaction
description The ethanol sensing properties of CuO nanowires prepared by oxidation reaction of copper plate have been examined. The characterization of CuO nanowires by FE-SEM, EDS, and TEM revealed diameters of 100-400 nm and a monoclinic structure with a growth direction along 〈1 1 0〉 direction. The ethanol sensing characteristics of CuO nanowires were studied at ethanol concentrations of 100-1000 ppm and working temperatures of 200-280 °C. An increase of resistance was observed under an ethanol vapor atmosphere due to the p-type semi-conducting property of CuO. It was found that the sensitivity, the response and the recovery time depended on the working temperatures and also ethanol concentration. The sensor exhibited the optimum sensitivity of 1.5 to ethanol vapor concentration of 1000 ppm at the working temperature of 240 °C with a response and recovery time of 110 and 120 s, respectively. © 2008 Elsevier Ltd and Techna Group S.r.l.
format Journal
author Phathaitep Raksa
Atcharawan Gardchareon
Torranin Chairuangsri
Pongsri Mangkorntong
Nikorn Mangkorntong
Supab Choopun
author_facet Phathaitep Raksa
Atcharawan Gardchareon
Torranin Chairuangsri
Pongsri Mangkorntong
Nikorn Mangkorntong
Supab Choopun
author_sort Phathaitep Raksa
title Ethanol sensing properties of CuO nanowires prepared by an oxidation reaction
title_short Ethanol sensing properties of CuO nanowires prepared by an oxidation reaction
title_full Ethanol sensing properties of CuO nanowires prepared by an oxidation reaction
title_fullStr Ethanol sensing properties of CuO nanowires prepared by an oxidation reaction
title_full_unstemmed Ethanol sensing properties of CuO nanowires prepared by an oxidation reaction
title_sort ethanol sensing properties of cuo nanowires prepared by an oxidation reaction
publishDate 2018
url https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=57749122161&origin=inward
http://cmuir.cmu.ac.th/jspui/handle/6653943832/59439