Microstuctural study and properties of 0.8PZT-0.2BT ceramics using a two-stage sintering procedure
Lead zirconate titanate-barium titanate (0.8PZT-0.2BT) ceramic was prepared by conventional mixed-oxide method combined with a two-stage sintering procedure. A sintering time of 2 h at 1000 °C followed by a second step in the temperature range of 1000-1200 °C for 2 h was employed to the samples and...
Saved in:
Main Author: | W. C. Vittayakorn |
---|---|
Format: | Book Series |
Published: |
2018
|
Subjects: | |
Online Access: | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=62949177297&origin=inward http://cmuir.cmu.ac.th/jspui/handle/6653943832/60361 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Chiang Mai University |
Similar Items
-
Microstuctural study and properties of 0.8PZT-0.2BT ceramics using a two-stage sintering procedure
by: Vittayakorn W.C.
Published: (2014) -
Composition, structure and properties of PZT-BT ceramics prepared by two-stage sintering
by: Vittayakorn W.C., et al.
Published: (2014) -
Composition, structure and properties of PZT-BT ceramics prepared by two-stage sintering
by: Wanwilai C. Vittayakorn, et al.
Published: (2018) -
Dielectric and ferroelectric properties of 0.8PZT-0.2PCN ceramics under sintering conditions variation
by: Anurak Prasatkhetragarn, et al.
Published: (2018) -
Dielectric and ferroelectric properties of 0.8PZT-0.2PCN ceramics under sintering conditions variation
by: Prasatkhetragarn A., et al.
Published: (2014)