Low sintering temperature of lead magnesium niobate-lead titanate (0.9PMN-0.1PT) by adding oxide additives

This research work is aimed at lowering the sintering temperature of 0.9PMN-0.1PT ceramics by adding oxide additives. The oxides used for this purpose were Bi2O3 and Li2CO3 with various amounts, following the formula of xBi2O3+yLi 2CO3, where x+y = 10 mol% and x = 1, 3, 5 and the mixed oxide additiv...