Effect of forming condition on compressive strength of hydroxyapatite-bioactive glass compact rod

© The Authors, published by EDP Sciences, 2018. With rising concerns regarding alloy implants, alternative biomaterials are currently studied, to avoid the adverse effects of metal on the human body such as irritation and inflammation. Hydroxyapatite (HA) and Bioactive glass (BG) are two bio-ceramic...

Full description

Saved in:
Bibliographic Details
Main Authors: Wassanai Wattanutchariya, Teerawat Sangkas
Format: Conference Proceeding
Published: 2018
Subjects:
Online Access:https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85053194411&origin=inward
http://cmuir.cmu.ac.th/jspui/handle/6653943832/62638
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Chiang Mai University
Description
Summary:© The Authors, published by EDP Sciences, 2018. With rising concerns regarding alloy implants, alternative biomaterials are currently studied, to avoid the adverse effects of metal on the human body such as irritation and inflammation. Hydroxyapatite (HA) and Bioactive glass (BG) are two bio-ceramics, which have been implemented in medical applications such as bone implants and fixation parts due to their biocompatibility and close resemblance to the mineralized phase of human bone. Furthermore, these materials can be synthesized from natural sources. In this study, M8 screws rod which are commonly implemented for bone fixation was selected as a case study to investigate an effect of forming conditions on the mechanical property of the composite structure. HA and BG were synthesized and formed into a composite specimen using a hydraulic pressing machine. Full factorial experimental design was employed to solve for an optimal forming condition. 3 factors consisting of mixing ratio, pressure and holding time for pressing were investigated for their impacts on the specimen's compressive strength. The result revealed that the BG ratio and pressure have a significant effect on the structural strength. The maximum compressive strength of 32.20 MPa was obtained from the specimen with 7.5 wt% of BG, 120 kg/cm2 of pressure and 30 second of holding time.