The Effect of Substitution of WC by TiC in WC-Co Composite Tool Materials on Microstructure and Mechanical Properties

WC-Co composites with TiC additions of 5-20 wt.% substituting WC were consolidated using Hot Isostatic Pressing (HIP) method at temperature of 1350°C and pressure between 50-150 MPa. The hardness of WC-Co consolidated samples increase from 1050 HV (without TiC consolidated at 50 MPa) up to 1330 HV...