Effects of annealing time on ferroelectric and piezoelectric properties of B2O3 doped Ba(Zr0.07Ti0.93)O 3 ceramics

The method of thermal annealing was applied to B2O3 doped BaZr0.07Ti0.93O3 ceramics. The modified ceramics were prepared via a solid state reaction method. The samples were sintered at 1250°C for 2 h, and then followed by the thermal annealing at 1000°C for 4-16 h to improve their electrical propert...