Improvement of electric field-induced strain and energy storage density properties in lead-free BNKT-based ceramics modified by BFT doping

© 2019 The Royal Society of Chemistry. In this research, the effects of Ba(Fe 0.5 Ta 0.5 )O 3 (BFT) additive on the phase evolution, the dielectric, ferroelectric, piezoelectric, electric field-induced strain responses, and energy storage density of the Bi 0.5 (Na 0.80 K 0.20 ) 0.5 TiO 3 -0.03(Ba 0...

Full description

Saved in:
Bibliographic Details
Main Authors: Pharatree Jaita, Ratabongkot Sanjoom, Narumon Lertcumfu, Gobwute Rujijanagul
Format: Journal
Published: 2019
Subjects:
Online Access:https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85064648278&origin=inward
http://cmuir.cmu.ac.th/jspui/handle/6653943832/65463
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Chiang Mai University
Description
Summary:© 2019 The Royal Society of Chemistry. In this research, the effects of Ba(Fe 0.5 Ta 0.5 )O 3 (BFT) additive on the phase evolution, the dielectric, ferroelectric, piezoelectric, electric field-induced strain responses, and energy storage density of the Bi 0.5 (Na 0.80 K 0.20 ) 0.5 TiO 3 -0.03(Ba 0.70 Sr 0.03 )TiO 3 (BNKT-0.03BSrT) ceramics have been systematically investigated. The ceramics have been prepared by a solid-state reaction method accompanied by two calcination steps. X-ray diffraction indicates that all ceramics coexist between rhombohedral and tetragonal phases, where the tetragonal phase becomes dominant at higher BFT contents. The addition of BFT also promotes the diffuse phase transition in this system. A significant enhancement of electric field-induced strain response (S max = 0.42% and = 840 pm V -1 ) is noted for the x = 0.01 ceramic. Furthermore, the giant electrostrictive coefficient (Q 33 = 0.0404 m 4 C -2 ) with a giant normalized electrostrictive coefficient (Q 33 /E = 8.08 × 10 -9 m 5 C -2 V -1 ) are also observed for this composition (x = 0.01). In addition, the x = 0.03 ceramic shows good energy storage properties, i.e. it has a high energy storage density (W = 0.65 J cm -3 @ 120 °C) with very high normalized storage energy density (W/E = 0.13 μC mm -2 ), and good energy storage efficiency (η = 90.4% @ 120 °C). Overall, these results indicate that these ceramics are one of the promising candidate piezoelectric materials for further development for actuator and high electric power pulse energy storage applications.