HRTEM and HAADF-STEM of precipitates at peak ageing of cast A319 aluminium alloy

High-resolution transmission electron microscopy (HRTEM) and high-angle annular-dark-field scanning transmission electron microscopy (HAADF-STEM) were applied to investigate the precipitates formed during age hardening at 170 ± 5 °C for up to 48. h of cast A319 aluminium alloy (Al-4.93. wt%Si-3.47....

Full description

Saved in:
Bibliographic Details
Main Authors: Wiengmoon A., Pearce J., Chairuangsri T., Isoda S., Saito H., Kurata H.
Format: Article
Language:English
Published: 2014
Online Access:http://www.scopus.com/inward/record.url?eid=2-s2.0-84872501027&partnerID=40&md5=7a64acc0aeb05a35c11a06a76ec9c4b9
http://cmuir.cmu.ac.th/handle/6653943832/6947
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Chiang Mai University
Language: English
id th-cmuir.6653943832-6947
record_format dspace
spelling th-cmuir.6653943832-69472014-08-30T03:51:25Z HRTEM and HAADF-STEM of precipitates at peak ageing of cast A319 aluminium alloy Wiengmoon A. Pearce J. Chairuangsri T. Isoda S. Saito H. Kurata H. High-resolution transmission electron microscopy (HRTEM) and high-angle annular-dark-field scanning transmission electron microscopy (HAADF-STEM) were applied to investigate the precipitates formed during age hardening at 170 ± 5 °C for up to 48. h of cast A319 aluminium alloy (Al-4.93. wt%Si-3.47. wt%Cu). The precipitates at the peak-aged condition have been identified as mainly θ" together with a smaller amount of θ'. It is proposed that the θ" is responsible for hardening at peak ageing at 170 °C of the cast A319 aluminium alloy. © 2012 Elsevier Ltd. 2014-08-30T03:51:25Z 2014-08-30T03:51:25Z 2013 Article 09684328 10.1016/j.micron.2012.10.009 MCONE http://www.scopus.com/inward/record.url?eid=2-s2.0-84872501027&partnerID=40&md5=7a64acc0aeb05a35c11a06a76ec9c4b9 http://cmuir.cmu.ac.th/handle/6653943832/6947 English
institution Chiang Mai University
building Chiang Mai University Library
country Thailand
collection CMU Intellectual Repository
language English
description High-resolution transmission electron microscopy (HRTEM) and high-angle annular-dark-field scanning transmission electron microscopy (HAADF-STEM) were applied to investigate the precipitates formed during age hardening at 170 ± 5 °C for up to 48. h of cast A319 aluminium alloy (Al-4.93. wt%Si-3.47. wt%Cu). The precipitates at the peak-aged condition have been identified as mainly θ" together with a smaller amount of θ'. It is proposed that the θ" is responsible for hardening at peak ageing at 170 °C of the cast A319 aluminium alloy. © 2012 Elsevier Ltd.
format Article
author Wiengmoon A.
Pearce J.
Chairuangsri T.
Isoda S.
Saito H.
Kurata H.
spellingShingle Wiengmoon A.
Pearce J.
Chairuangsri T.
Isoda S.
Saito H.
Kurata H.
HRTEM and HAADF-STEM of precipitates at peak ageing of cast A319 aluminium alloy
author_facet Wiengmoon A.
Pearce J.
Chairuangsri T.
Isoda S.
Saito H.
Kurata H.
author_sort Wiengmoon A.
title HRTEM and HAADF-STEM of precipitates at peak ageing of cast A319 aluminium alloy
title_short HRTEM and HAADF-STEM of precipitates at peak ageing of cast A319 aluminium alloy
title_full HRTEM and HAADF-STEM of precipitates at peak ageing of cast A319 aluminium alloy
title_fullStr HRTEM and HAADF-STEM of precipitates at peak ageing of cast A319 aluminium alloy
title_full_unstemmed HRTEM and HAADF-STEM of precipitates at peak ageing of cast A319 aluminium alloy
title_sort hrtem and haadf-stem of precipitates at peak ageing of cast a319 aluminium alloy
publishDate 2014
url http://www.scopus.com/inward/record.url?eid=2-s2.0-84872501027&partnerID=40&md5=7a64acc0aeb05a35c11a06a76ec9c4b9
http://cmuir.cmu.ac.th/handle/6653943832/6947
_version_ 1681420709113364480