Thermal expansion behavior of (Bi0.5Na0.5)Zr 1- xTix O3 ceramics

(Bi0.5Na0.5)Zr1-xTixO 3 with x = 0, 0.1, 0.2, 0.3, 0.4, 0.5 and 0.6 ceramics were fabricated by a conventional sintering technique at 850-950°C for 2 h. From X-ray diffraction study, three regions of different phases were observed in the ceramic system; i.e., orthorhombic phase region (0 ≤ x ≤ 0.2),...