Preparation and characterization of BiVO4 powder by the sol-gel method

Bismuth vanadate (BiVO4) powder was successfully prepared by the sol-gel method. Bismuth nitrate and ammonium vanadate were used as the starting precursors with mole ratio of 1:1 in ethanol media at 70°C for 1 h. The yellow gel was calcined at 400-600°C for 2 h. The phase of BiVO4 powder was charact...

Full description

Saved in:
Bibliographic Details
Main Authors: Pookmanee P., Kojinok S., Puntharod R., Sangsrichan S., Phanichphant S.
Format: Article
Language:English
Published: 2014
Online Access:http://www.scopus.com/inward/record.url?eid=2-s2.0-84891754654&partnerID=40&md5=f6f07ca9428453e1b6052c5971915420
http://cmuir.cmu.ac.th/handle/6653943832/7322
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Chiang Mai University
Language: English
Description
Summary:Bismuth vanadate (BiVO4) powder was successfully prepared by the sol-gel method. Bismuth nitrate and ammonium vanadate were used as the starting precursors with mole ratio of 1:1 in ethanol media at 70°C for 1 h. The yellow gel was calcined at 400-600°C for 2 h. The phase of BiVO4 powder was characterized by X-ray diffraction (XRD). The morphology and chemical composition of BiVO4 powder were investigated by scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDXS). The functional groups of BiVO4 powder was identified by Fourier transform infrared spectroscopy (FTIR) and the surface area of BiVO4 powder was determined by Brunauer, Emmett and Teller technique (BET). © 2013 Copyright Taylor and Francis Group, LLC.