Shear and micro-shear bond strengths of four self-etching adhesives measured immediately and 24 hours after application
This study measured the immediate and 24 h shear (SBS) and micro-shear bond strengths (MSBS) to dentin of four self-etching adhesives. A resin composite was bonded using each adhesive to the area of 5-mm diameter for SBS test or 0.75-mm diameter for MSBS test of flat bovine dentin. The bond strength...
Saved in:
Main Authors: | , , , |
---|---|
Other Authors: | |
Format: | Article |
Published: |
2018
|
Subjects: | |
Online Access: | https://repository.li.mahidol.ac.th/handle/123456789/14072 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Mahidol University |
id |
th-mahidol.14072 |
---|---|
record_format |
dspace |
spelling |
th-mahidol.140722018-06-11T11:55:37Z Shear and micro-shear bond strengths of four self-etching adhesives measured immediately and 24 hours after application Choltacha Harnirattisai Panitta Roengrungreang Utumporn Rangsisiripaiboon Pisol Senawongse Mahidol University Thailand Ministry of Public Health Dentistry Materials Science This study measured the immediate and 24 h shear (SBS) and micro-shear bond strengths (MSBS) to dentin of four self-etching adhesives. A resin composite was bonded using each adhesive to the area of 5-mm diameter for SBS test or 0.75-mm diameter for MSBS test of flat bovine dentin. The bond strengths of all adhesives at 10 min were lower than at 24 h for both tests. The mean SBS (MPa, 10 min, 24 h) were similar in ranking order at both time periods that is: Clearfil SE Bond (21.2, 25.3) > Clearfil TriS Bond (12.7, 19.5)=i Bond (11.7, 19.5)=G Bond (11.1, 16.6). For the MSBS test, G Bond provided equivalent mean bond strength (35.0) to Clearfil SE Bond (36.9) and higher than the other adhesives at 24 h [i Bond (26.3), Clearfil TriS Bond (28.5)]. In conclusion, the MSBS test was slightly more discriminating than the SBS test. 2018-06-11T04:46:13Z 2018-06-11T04:46:13Z 2012-10-30 Article Dental Materials Journal. Vol.31, No.5 (2012), 779-787 10.4012/dmj.2012-013 18811361 02874547 2-s2.0-84867862374 https://repository.li.mahidol.ac.th/handle/123456789/14072 Mahidol University SCOPUS https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84867862374&origin=inward |
institution |
Mahidol University |
building |
Mahidol University Library |
continent |
Asia |
country |
Thailand Thailand |
content_provider |
Mahidol University Library |
collection |
Mahidol University Institutional Repository |
topic |
Dentistry Materials Science |
spellingShingle |
Dentistry Materials Science Choltacha Harnirattisai Panitta Roengrungreang Utumporn Rangsisiripaiboon Pisol Senawongse Shear and micro-shear bond strengths of four self-etching adhesives measured immediately and 24 hours after application |
description |
This study measured the immediate and 24 h shear (SBS) and micro-shear bond strengths (MSBS) to dentin of four self-etching adhesives. A resin composite was bonded using each adhesive to the area of 5-mm diameter for SBS test or 0.75-mm diameter for MSBS test of flat bovine dentin. The bond strengths of all adhesives at 10 min were lower than at 24 h for both tests. The mean SBS (MPa, 10 min, 24 h) were similar in ranking order at both time periods that is: Clearfil SE Bond (21.2, 25.3) > Clearfil TriS Bond (12.7, 19.5)=i Bond (11.7, 19.5)=G Bond (11.1, 16.6). For the MSBS test, G Bond provided equivalent mean bond strength (35.0) to Clearfil SE Bond (36.9) and higher than the other adhesives at 24 h [i Bond (26.3), Clearfil TriS Bond (28.5)]. In conclusion, the MSBS test was slightly more discriminating than the SBS test. |
author2 |
Mahidol University |
author_facet |
Mahidol University Choltacha Harnirattisai Panitta Roengrungreang Utumporn Rangsisiripaiboon Pisol Senawongse |
format |
Article |
author |
Choltacha Harnirattisai Panitta Roengrungreang Utumporn Rangsisiripaiboon Pisol Senawongse |
author_sort |
Choltacha Harnirattisai |
title |
Shear and micro-shear bond strengths of four self-etching adhesives measured immediately and 24 hours after application |
title_short |
Shear and micro-shear bond strengths of four self-etching adhesives measured immediately and 24 hours after application |
title_full |
Shear and micro-shear bond strengths of four self-etching adhesives measured immediately and 24 hours after application |
title_fullStr |
Shear and micro-shear bond strengths of four self-etching adhesives measured immediately and 24 hours after application |
title_full_unstemmed |
Shear and micro-shear bond strengths of four self-etching adhesives measured immediately and 24 hours after application |
title_sort |
shear and micro-shear bond strengths of four self-etching adhesives measured immediately and 24 hours after application |
publishDate |
2018 |
url |
https://repository.li.mahidol.ac.th/handle/123456789/14072 |
_version_ |
1763488519297171456 |