Bio-reduced Ag nanoparticle decorated on ZnO for enhancement of photocatalytic reduction of hexavalent chromium and photocatalytic degradation of rhodamine B

Ag nanoparticles reduced by organic components extracted from Jasmine tea leaves were decorated by a hydrothermal reaction on ZnO to fabricate AgNPs@ZnO composite, and then the composite was applied for photocatalytic reactions to degrade rhodamine B (RhB) and reduce hexavalent chromium (Cr(VI)). Th...

Full description

Saved in:
Bibliographic Details
Main Author: Chuaicham C.
Other Authors: Mahidol University
Format: Article
Published: 2023
Subjects:
Online Access:https://repository.li.mahidol.ac.th/handle/123456789/80184
https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85146190408&origin=inward
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Mahidol University
id th-mahidol.80184
record_format dspace
spelling th-mahidol.801842023-02-10T07:01:29Z Bio-reduced Ag nanoparticle decorated on ZnO for enhancement of photocatalytic reduction of hexavalent chromium and photocatalytic degradation of rhodamine B Chuaicham C. Mahidol University Engineering Ag nanoparticles reduced by organic components extracted from Jasmine tea leaves were decorated by a hydrothermal reaction on ZnO to fabricate AgNPs@ZnO composite, and then the composite was applied for photocatalytic reactions to degrade rhodamine B (RhB) and reduce hexavalent chromium (Cr(VI)). The produced composite (AgNPs@ZnO) was optically and physicochemically characterized to better understand the impact of the development of the AgNPs-ZnO heterojunction when compared to that of pure ZnO. The optimized AgNPs@ZnO reduced more than 95% of 10 mg/L Cr(VI) in 60 min and degraded more than 95% of 10 mg/L RhB in 180 min, with a rate constant around five times for Cr reduction and three times for RhB degradation faster than that of pure ZnO, due to its superior capacity to separate and transport photogenerated electron-hole pairs, as evidenced by a drop in photoluminescence intensity. Furthermore, when AgNPs were placed on the surface of ZnO in the composites, surface defects were generated on ZnO, as confirmed by the energy-resolved distribution of electron trap (ERDT) pattern for AgNPs@ZnO, indicating the formation of new electron trapping levels. This might cause a reduction of the energy band gap, resulting in the enhancement of light adsorption and reduction of charge recombination. Therefore, the present bio-induced composite of AgNPs@ZnO opens up new possibilities for photochemical purification technology in aquatic environments. 2023-02-10T00:01:29Z 2023-02-10T00:01:29Z 2023-04-05 Article Journal of Alloys and Compounds Vol.939 (2023) 10.1016/j.jallcom.2023.168797 09258388 2-s2.0-85146190408 https://repository.li.mahidol.ac.th/handle/123456789/80184 https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85146190408&origin=inward SCOPUS
institution Mahidol University
building Mahidol University Library
continent Asia
country Thailand
Thailand
content_provider Mahidol University Library
collection Mahidol University Institutional Repository
topic Engineering
spellingShingle Engineering
Chuaicham C.
Bio-reduced Ag nanoparticle decorated on ZnO for enhancement of photocatalytic reduction of hexavalent chromium and photocatalytic degradation of rhodamine B
description Ag nanoparticles reduced by organic components extracted from Jasmine tea leaves were decorated by a hydrothermal reaction on ZnO to fabricate AgNPs@ZnO composite, and then the composite was applied for photocatalytic reactions to degrade rhodamine B (RhB) and reduce hexavalent chromium (Cr(VI)). The produced composite (AgNPs@ZnO) was optically and physicochemically characterized to better understand the impact of the development of the AgNPs-ZnO heterojunction when compared to that of pure ZnO. The optimized AgNPs@ZnO reduced more than 95% of 10 mg/L Cr(VI) in 60 min and degraded more than 95% of 10 mg/L RhB in 180 min, with a rate constant around five times for Cr reduction and three times for RhB degradation faster than that of pure ZnO, due to its superior capacity to separate and transport photogenerated electron-hole pairs, as evidenced by a drop in photoluminescence intensity. Furthermore, when AgNPs were placed on the surface of ZnO in the composites, surface defects were generated on ZnO, as confirmed by the energy-resolved distribution of electron trap (ERDT) pattern for AgNPs@ZnO, indicating the formation of new electron trapping levels. This might cause a reduction of the energy band gap, resulting in the enhancement of light adsorption and reduction of charge recombination. Therefore, the present bio-induced composite of AgNPs@ZnO opens up new possibilities for photochemical purification technology in aquatic environments.
author2 Mahidol University
author_facet Mahidol University
Chuaicham C.
format Article
author Chuaicham C.
author_sort Chuaicham C.
title Bio-reduced Ag nanoparticle decorated on ZnO for enhancement of photocatalytic reduction of hexavalent chromium and photocatalytic degradation of rhodamine B
title_short Bio-reduced Ag nanoparticle decorated on ZnO for enhancement of photocatalytic reduction of hexavalent chromium and photocatalytic degradation of rhodamine B
title_full Bio-reduced Ag nanoparticle decorated on ZnO for enhancement of photocatalytic reduction of hexavalent chromium and photocatalytic degradation of rhodamine B
title_fullStr Bio-reduced Ag nanoparticle decorated on ZnO for enhancement of photocatalytic reduction of hexavalent chromium and photocatalytic degradation of rhodamine B
title_full_unstemmed Bio-reduced Ag nanoparticle decorated on ZnO for enhancement of photocatalytic reduction of hexavalent chromium and photocatalytic degradation of rhodamine B
title_sort bio-reduced ag nanoparticle decorated on zno for enhancement of photocatalytic reduction of hexavalent chromium and photocatalytic degradation of rhodamine b
publishDate 2023
url https://repository.li.mahidol.ac.th/handle/123456789/80184
https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85146190408&origin=inward
_version_ 1763490950755123200