KAJIAN EKSPERIMENTAL PERILAKU KERUNTUHAN BALOK MENERUS DENGAN DIISI POLIMER

Four continuous beams were tested to failure under third point loading. These beams were 2800 mm long and had two equal 1300 mm clear spans, with a rectangular section 100 mm wide by 150 mm deep. Two of them, with compressive strength of 30 MPa and 50 MPa, had void 3 mm filled with polymer matrix. T...