PENGEMBANGAN FORMULA SCAFFOLD BIONANOKOMPOSIT KITOSAN UNTUK IMPLAN TULANG

Tissue engineering is an alternatives method in treating bone injure by induction of tissue to naturally regenerate. Regeneration of bone and cartilage injure can be accelerated by localized delivery of a dosage form with growth factors incorporated within biodegradable carrier. Carrier is an extrac...

Full description

Saved in:
Bibliographic Details
Main Author: Ramadhan, Pradipta
Format: Final Project
Language:Indonesia
Online Access:https://digilib.itb.ac.id/gdl/view/64302
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Institut Teknologi Bandung
Language: Indonesia
id id-itb.:64302
spelling id-itb.:643022022-05-10T14:37:33ZPENGEMBANGAN FORMULA SCAFFOLD BIONANOKOMPOSIT KITOSAN UNTUK IMPLAN TULANG Ramadhan, Pradipta Indonesia Final Project - INSTITUT TEKNOLOGI BANDUNG https://digilib.itb.ac.id/gdl/view/64302 Tissue engineering is an alternatives method in treating bone injure by induction of tissue to naturally regenerate. Regeneration of bone and cartilage injure can be accelerated by localized delivery of a dosage form with growth factors incorporated within biodegradable carrier. Carrier is an extracellular matrix that serves as a temporary replacement for damaged tissue called scaffold. Scaffold materials used are chitosan because of its biocompatibility, osteoconductivity and biodegradable. However, chitosan has low mechanical strength, therefore it takes the addition of hydroxyapatite ceramics is needed to increase the mechanical strength. This research was make matrix formulation with model protein and its characterization and evaluation. Scaffold is carrying a growth factor protein, then the process of solid dispersions and lyophilized of protein to maintain its stability are needed. Solid dispersion of protein were prepared by addition of polyethylene glycol (PEG) 20.000 to improve protein solubility in oil phase. Virgin coconut oil (VCO) was used for oil phase with addition of Tween 80 as surfactant and PEG 400 as co-surfactant. Bovine serum albumin (BSA) was choosen as protein model instead of growth factor. Then oil phase was mixed with chitosan solution as water phase to form oil in water emulsion system. In addition, solid dispersion of nanohydroxyapatite that stabilized by sodium carboxymetyl celulose (CMC-Na) were added into the system. The mixture was then extruded into sodium tripolyphosphate (STPP) 5% w/v solution for crosslinking. Microspheres were observed including to morphology, size distribution, and protein entrapment efficiency. After that it's packed to obtain a 3 dimensional matrix to characterized including to density, porosity, protein release study, and mechanical strength. Entrapment efficiency of proteins by solid dispersion using PEG 20,000 with the ratio 1:1 was 98.99%. Size of the mierospheres were in the range 800-1.000 um. And the total concentration of the release of the scaffold was 75,4 ug/mL or 22.8 % for 4 weeks test. Mechanical strength from matrix was 0.32 MPa. The best scaffold formulation was solid dispersion of protein with PEG 20.000 with the ratio 1:1 because its entrapment efficiency was 98.99 ± 0.087% and release study for four weeks test was 22.8 %. text
institution Institut Teknologi Bandung
building Institut Teknologi Bandung Library
continent Asia
country Indonesia
Indonesia
content_provider Institut Teknologi Bandung
collection Digital ITB
language Indonesia
description Tissue engineering is an alternatives method in treating bone injure by induction of tissue to naturally regenerate. Regeneration of bone and cartilage injure can be accelerated by localized delivery of a dosage form with growth factors incorporated within biodegradable carrier. Carrier is an extracellular matrix that serves as a temporary replacement for damaged tissue called scaffold. Scaffold materials used are chitosan because of its biocompatibility, osteoconductivity and biodegradable. However, chitosan has low mechanical strength, therefore it takes the addition of hydroxyapatite ceramics is needed to increase the mechanical strength. This research was make matrix formulation with model protein and its characterization and evaluation. Scaffold is carrying a growth factor protein, then the process of solid dispersions and lyophilized of protein to maintain its stability are needed. Solid dispersion of protein were prepared by addition of polyethylene glycol (PEG) 20.000 to improve protein solubility in oil phase. Virgin coconut oil (VCO) was used for oil phase with addition of Tween 80 as surfactant and PEG 400 as co-surfactant. Bovine serum albumin (BSA) was choosen as protein model instead of growth factor. Then oil phase was mixed with chitosan solution as water phase to form oil in water emulsion system. In addition, solid dispersion of nanohydroxyapatite that stabilized by sodium carboxymetyl celulose (CMC-Na) were added into the system. The mixture was then extruded into sodium tripolyphosphate (STPP) 5% w/v solution for crosslinking. Microspheres were observed including to morphology, size distribution, and protein entrapment efficiency. After that it's packed to obtain a 3 dimensional matrix to characterized including to density, porosity, protein release study, and mechanical strength. Entrapment efficiency of proteins by solid dispersion using PEG 20,000 with the ratio 1:1 was 98.99%. Size of the mierospheres were in the range 800-1.000 um. And the total concentration of the release of the scaffold was 75,4 ug/mL or 22.8 % for 4 weeks test. Mechanical strength from matrix was 0.32 MPa. The best scaffold formulation was solid dispersion of protein with PEG 20.000 with the ratio 1:1 because its entrapment efficiency was 98.99 ± 0.087% and release study for four weeks test was 22.8 %.
format Final Project
author Ramadhan, Pradipta
spellingShingle Ramadhan, Pradipta
PENGEMBANGAN FORMULA SCAFFOLD BIONANOKOMPOSIT KITOSAN UNTUK IMPLAN TULANG
author_facet Ramadhan, Pradipta
author_sort Ramadhan, Pradipta
title PENGEMBANGAN FORMULA SCAFFOLD BIONANOKOMPOSIT KITOSAN UNTUK IMPLAN TULANG
title_short PENGEMBANGAN FORMULA SCAFFOLD BIONANOKOMPOSIT KITOSAN UNTUK IMPLAN TULANG
title_full PENGEMBANGAN FORMULA SCAFFOLD BIONANOKOMPOSIT KITOSAN UNTUK IMPLAN TULANG
title_fullStr PENGEMBANGAN FORMULA SCAFFOLD BIONANOKOMPOSIT KITOSAN UNTUK IMPLAN TULANG
title_full_unstemmed PENGEMBANGAN FORMULA SCAFFOLD BIONANOKOMPOSIT KITOSAN UNTUK IMPLAN TULANG
title_sort pengembangan formula scaffold bionanokomposit kitosan untuk implan tulang
url https://digilib.itb.ac.id/gdl/view/64302
_version_ 1822276973652606976