SINTESIS DAN KARAKTERISASI KOMPOSIT KITOSAN-ZEOLIT TERAKTIVASI BASA-Fe SEBAGAI SISTEM LEPAS LAMBAT Fe(III)

Preparation of an iron (III) slow release materials using chitosan and alkaline activated zeolite and evaluation of their release behaviour in the 0.33 M citric acid solution have been done. The composites were prepared by mixing chitosan gel, alkaline activated zeolite, and FeSO4 solution. Then the...

Full description

Saved in:
Bibliographic Details
Main Authors: , Ratu Fazlia Inda Rahmayani, , Dr. Yateman Arryanto
Format: Theses and Dissertations NonPeerReviewed
Published: [Yogyakarta] : Universitas Gadjah Mada 2014
Subjects:
ETD
Online Access:https://repository.ugm.ac.id/129914/
http://etd.ugm.ac.id/index.php?mod=penelitian_detail&sub=PenelitianDetail&act=view&typ=html&buku_id=70323
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Universitas Gadjah Mada
id id-ugm-repo.129914
record_format dspace
spelling id-ugm-repo.1299142016-03-04T08:11:08Z https://repository.ugm.ac.id/129914/ SINTESIS DAN KARAKTERISASI KOMPOSIT KITOSAN-ZEOLIT TERAKTIVASI BASA-Fe SEBAGAI SISTEM LEPAS LAMBAT Fe(III) , Ratu Fazlia Inda Rahmayani , Dr. Yateman Arryanto ETD Preparation of an iron (III) slow release materials using chitosan and alkaline activated zeolite and evaluation of their release behaviour in the 0.33 M citric acid solution have been done. The composites were prepared by mixing chitosan gel, alkaline activated zeolite, and FeSO4 solution. Then the mixture was dripped into NaOH solution. Composite synthesis was carried out by varying the consentration of NaOH for zeolite activation. The structure of composite was characterized using infrared spectrophotometer and X-Ray diffractometer. The surface morphology of composite was analyzed using SEM and the thermal stabilities were analyzed using TGA. The result of composite, with variation in mixing methode, releasing evaluation didn�t show any difference in releasing behaviour, so that the composite made by mixing the zeolite and Fe previously then chitosan (composite C) was selected as the representatif of the other composites. Evaluation of release in the 0.33 M citric acid for composite from consentration variation of NaOH showed that the release order of Fe(III) is the composite C (6 M) > composite C (4 M) > Composite C (2 M) > composite C (0 M) with values of k are 0.021 mg/g [Yogyakarta] : Universitas Gadjah Mada 2014 Thesis NonPeerReviewed , Ratu Fazlia Inda Rahmayani and , Dr. Yateman Arryanto (2014) SINTESIS DAN KARAKTERISASI KOMPOSIT KITOSAN-ZEOLIT TERAKTIVASI BASA-Fe SEBAGAI SISTEM LEPAS LAMBAT Fe(III). UNSPECIFIED thesis, UNSPECIFIED. http://etd.ugm.ac.id/index.php?mod=penelitian_detail&sub=PenelitianDetail&act=view&typ=html&buku_id=70323
institution Universitas Gadjah Mada
building UGM Library
country Indonesia
collection Repository Civitas UGM
topic ETD
spellingShingle ETD
, Ratu Fazlia Inda Rahmayani
, Dr. Yateman Arryanto
SINTESIS DAN KARAKTERISASI KOMPOSIT KITOSAN-ZEOLIT TERAKTIVASI BASA-Fe SEBAGAI SISTEM LEPAS LAMBAT Fe(III)
description Preparation of an iron (III) slow release materials using chitosan and alkaline activated zeolite and evaluation of their release behaviour in the 0.33 M citric acid solution have been done. The composites were prepared by mixing chitosan gel, alkaline activated zeolite, and FeSO4 solution. Then the mixture was dripped into NaOH solution. Composite synthesis was carried out by varying the consentration of NaOH for zeolite activation. The structure of composite was characterized using infrared spectrophotometer and X-Ray diffractometer. The surface morphology of composite was analyzed using SEM and the thermal stabilities were analyzed using TGA. The result of composite, with variation in mixing methode, releasing evaluation didn�t show any difference in releasing behaviour, so that the composite made by mixing the zeolite and Fe previously then chitosan (composite C) was selected as the representatif of the other composites. Evaluation of release in the 0.33 M citric acid for composite from consentration variation of NaOH showed that the release order of Fe(III) is the composite C (6 M) > composite C (4 M) > Composite C (2 M) > composite C (0 M) with values of k are 0.021 mg/g
format Theses and Dissertations
NonPeerReviewed
author , Ratu Fazlia Inda Rahmayani
, Dr. Yateman Arryanto
author_facet , Ratu Fazlia Inda Rahmayani
, Dr. Yateman Arryanto
author_sort , Ratu Fazlia Inda Rahmayani
title SINTESIS DAN KARAKTERISASI KOMPOSIT KITOSAN-ZEOLIT TERAKTIVASI BASA-Fe SEBAGAI SISTEM LEPAS LAMBAT Fe(III)
title_short SINTESIS DAN KARAKTERISASI KOMPOSIT KITOSAN-ZEOLIT TERAKTIVASI BASA-Fe SEBAGAI SISTEM LEPAS LAMBAT Fe(III)
title_full SINTESIS DAN KARAKTERISASI KOMPOSIT KITOSAN-ZEOLIT TERAKTIVASI BASA-Fe SEBAGAI SISTEM LEPAS LAMBAT Fe(III)
title_fullStr SINTESIS DAN KARAKTERISASI KOMPOSIT KITOSAN-ZEOLIT TERAKTIVASI BASA-Fe SEBAGAI SISTEM LEPAS LAMBAT Fe(III)
title_full_unstemmed SINTESIS DAN KARAKTERISASI KOMPOSIT KITOSAN-ZEOLIT TERAKTIVASI BASA-Fe SEBAGAI SISTEM LEPAS LAMBAT Fe(III)
title_sort sintesis dan karakterisasi komposit kitosan-zeolit teraktivasi basa-fe sebagai sistem lepas lambat fe(iii)
publisher [Yogyakarta] : Universitas Gadjah Mada
publishDate 2014
url https://repository.ugm.ac.id/129914/
http://etd.ugm.ac.id/index.php?mod=penelitian_detail&sub=PenelitianDetail&act=view&typ=html&buku_id=70323
_version_ 1681233057295630336