Study of fabrication Al-Tin slag composite by powder metallurgy method
In the present investigation, Aluminum-tin slag composite have been produced by powder metallurgy (P/M) route. Aluminum (Al) and tin slag were undergo milling and sieving process where particle size <75 µm and <63 µm for tin slag and aluminum were obtained. Both Al and tin slag were mixed f...
Saved in:
Main Author: | |
---|---|
Other Authors: | |
Format: | Learning Object |
Language: | English |
Published: |
Universiti Malaysia Perlis
2008
|
Subjects: | |
Online Access: | http://dspace.unimap.edu.my/xmlui/handle/123456789/3350 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Universiti Malaysia Perlis |
Language: | English |
id |
my.unimap-3350 |
---|---|
record_format |
dspace |
spelling |
my.unimap-33502008-11-26T05:07:22Z Study of fabrication Al-Tin slag composite by powder metallurgy method Muhamad Syazwan Abdul Manan Mohd Fitri Mohamad Wahid (Advisor) Aluminum Aluminum composites Aluminum -- Mechanical properties Powder metallurgy Tin slag Aluminum matrix composite In the present investigation, Aluminum-tin slag composite have been produced by powder metallurgy (P/M) route. Aluminum (Al) and tin slag were undergo milling and sieving process where particle size <75 µm and <63 µm for tin slag and aluminum were obtained. Both Al and tin slag were mixed for 40 minutes with a speed of 100rpm. Both of the Al and tin slag powder were mixed by weight percent which is Al-5% of tin slag, Al-10% of tin slag, Al-15% of tin slag and Al-20% of tin slag correspond to sample A, B, C, D respectively. Samples were compacted with the load of 5 tonne (180 Mpa) for 3 minutes. The samples were placed in a tube furnace with nitrogen, N2 purified atmosphere at 600oC for 7 hours soaking time, with heating and cooling rate of 5oC/ min for 1 hour and 9 minutes respectively. Mechanical properties like shrinkage, hardness, density and porosity of Al-tin slag composite were investigated. All the samples experienced shrinkage. In increase addition of tin slag, hardness and density value was also increased. % of porosity decreased with the increased addition of tin slag. Microstructures of Al-tin slag composite were also investigated. The microstructure of this Al-tin slag composite shows a uniform distribution of tin slag in the Al matrix. 2008-11-26T05:07:22Z 2008-11-26T05:07:22Z 2008-05 Learning Object http://hdl.handle.net/123456789/3350 en Universiti Malaysia Perlis School of Materials Engineering |
institution |
Universiti Malaysia Perlis |
building |
UniMAP Library |
collection |
Institutional Repository |
continent |
Asia |
country |
Malaysia |
content_provider |
Universiti Malaysia Perlis |
content_source |
UniMAP Library Digital Repository |
url_provider |
http://dspace.unimap.edu.my/ |
language |
English |
topic |
Aluminum Aluminum composites Aluminum -- Mechanical properties Powder metallurgy Tin slag Aluminum matrix composite |
spellingShingle |
Aluminum Aluminum composites Aluminum -- Mechanical properties Powder metallurgy Tin slag Aluminum matrix composite Muhamad Syazwan Abdul Manan Study of fabrication Al-Tin slag composite by powder metallurgy method |
description |
In the present investigation, Aluminum-tin slag composite have been produced by powder
metallurgy (P/M) route. Aluminum (Al) and tin slag were undergo milling and sieving
process where particle size <75 µm and <63 µm for tin slag and aluminum were obtained.
Both Al and tin slag were mixed for 40 minutes with a speed of 100rpm. Both of the Al and tin slag powder were mixed by weight percent which is Al-5% of tin slag, Al-10% of tin slag, Al-15% of tin slag and Al-20% of tin slag correspond to sample A, B, C, D
respectively. Samples were compacted with the load of 5 tonne (180 Mpa) for 3 minutes.
The samples were placed in a tube furnace with nitrogen, N2 purified atmosphere at 600oC for 7 hours soaking time, with heating and cooling rate of 5oC/ min for 1 hour and 9
minutes respectively. Mechanical properties like shrinkage, hardness, density and porosity of Al-tin slag composite were investigated. All the samples experienced shrinkage. In increase addition of tin slag, hardness and density value was also increased. % of porosity decreased with the increased addition of tin slag. Microstructures of Al-tin slag composite
were also investigated. The microstructure of this Al-tin slag composite shows a uniform
distribution of tin slag in the Al matrix. |
author2 |
Mohd Fitri Mohamad Wahid (Advisor) |
author_facet |
Mohd Fitri Mohamad Wahid (Advisor) Muhamad Syazwan Abdul Manan |
format |
Learning Object |
author |
Muhamad Syazwan Abdul Manan |
author_sort |
Muhamad Syazwan Abdul Manan |
title |
Study of fabrication Al-Tin slag composite by powder metallurgy method |
title_short |
Study of fabrication Al-Tin slag composite by powder metallurgy method |
title_full |
Study of fabrication Al-Tin slag composite by powder metallurgy method |
title_fullStr |
Study of fabrication Al-Tin slag composite by powder metallurgy method |
title_full_unstemmed |
Study of fabrication Al-Tin slag composite by powder metallurgy method |
title_sort |
study of fabrication al-tin slag composite by powder metallurgy method |
publisher |
Universiti Malaysia Perlis |
publishDate |
2008 |
url |
http://dspace.unimap.edu.my/xmlui/handle/123456789/3350 |
_version_ |
1643787870118346752 |