Enhancement of thermal and mechanical stabilities of silicon doped titanium nitride coating by manipulation of sputtering conditions

This study investigates the influence of substrate (AISI M42 tool steel) bias voltage (from −30 to −80 V), on the mechanical properties of magnetron sputtered TiSiN coating derived from Ti and Si targets. Thermal stability, microstructure (crystallite size, microstrain, lattice constant), morphology...

Full description

Saved in:
Bibliographic Details
Main Authors: Mohammadpour, Ehsan, Yun, Willey Hsien Liew, Mondinos, Nicholas, Altarawneh, Mohammednoor, Lee, Sunghwan, Radevski, Nik, Minakshi, Manickam, Amri, Amun, Lim, Hong Ngee, Jiang, Zhong Tao
Format: Article
Published: Elsevier 2022
Online Access:http://psasir.upm.edu.my/id/eprint/101268/
https://www.sciencedirect.com/science/article/pii/S2238785422000394
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Universiti Putra Malaysia
Description
Summary:This study investigates the influence of substrate (AISI M42 tool steel) bias voltage (from −30 to −80 V), on the mechanical properties of magnetron sputtered TiSiN coating derived from Ti and Si targets. Thermal stability, microstructure (crystallite size, microstrain, lattice constant), morphology and mechanical (hardness, Young's modulus, residual stresses) properties, of the deposited TiSiN coatings, were investigated with synchrotron powered X-ray diffraction (SR-XRD), X-ray photoelectron spectroscopy, field emission scanning electron microscopy, and nanoindentation techniques. Rietveld analysis, of the in-situ SR-XRD, in the temperature range of 25–800 °C, demonstrated cubic TiN form in (Ti,Si)N solid solutions, with TiO2 and Ti2O3 identified at lower bias voltages. Density functional theory supplemented the experimental results. Increase in the bias voltage resulted in: (i) a decrease in Si content, (ii) significant smoothening of surface morphology, (iii) change in the phase composition and microstructure, (iv) improved oxidation resistance and thermal oxidation threshold, and (v) hardness and Young's modulus of the coatings increased up to 50% to 33 GPa and 450 GPa, respectively.