Tough and dense boron carbide obtained by high-pressure (300 MPa) and low-temperature (1600°C) spark plasma sintering

Dense boron carbide (above 95%) was achieved through high pressure (300 MPa) and low temperature (1600°C) Spark Plasma Sintering (SPS). This approach resulted in improvement of fracture toughness and of dynamic toughness when compared to corresponding toughness values of the sample sintered by conve...