Tough and dense boron carbide obtained by high-pressure (300 MPa) and low-temperature (1600°C) spark plasma sintering
Dense boron carbide (above 95%) was achieved through high pressure (300 MPa) and low temperature (1600°C) Spark Plasma Sintering (SPS). This approach resulted in improvement of fracture toughness and of dynamic toughness when compared to corresponding toughness values of the sample sintered by conve...
Saved in:
Main Authors: | Badica, Petre, Grasso, Salvatore, Borodianska, Hanna, Xie, Sky Shumao, Li, Peifeng, Tatarko, Peter, Reece, Mike J., Sakka, Yoshio, Vasylkiv, Oleg |
---|---|
Other Authors: | Temasek Laboratories |
Format: | Article |
Language: | English |
Published: |
2014
|
Subjects: | |
Online Access: | https://hdl.handle.net/10356/105276 http://hdl.handle.net/10220/20506 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Nanyang Technological University |
Language: | English |
Similar Items
-
B6O ceramic by in-situ reactive spark plasma sintering of a B2O3 and B powder mixture
by: Sakka, Yoshio, et al.
Published: (2014) -
Grain boundary diffusion driven spark plasma sintering of nanocrystalline zirconia
by: Borodianska, Hanna, et al.
Published: (2013) -
Metal-ceramic/ceramic nanostructured layered composites for solid oxide fuel cells by spark plasma sintering
by: Bezdorozhev, Oleksii, et al.
Published: (2014) -
Spark plasma sintered Ni-YSZ/YSZ bi-layers for solid oxide fuel cell
by: Bezdorozhev, Oleksii, et al.
Published: (2014) -
Bio-inspired structured boron carbide-boron nitride composite by reactive spark plasma sintering
by: Silberschmidt, V., et al.
Published: (2014)