Vacuum brazing of dissimilar Al 7075 and Al–25 Si alloy
The vacuum brazing of dissimilar Al 7075 and Al–25 Si alloy was investigated. The brazing filler was copper foil with a thickness of 20 µm, and the brazing temperature was 560◦ C held for 10 min. The average shear strength of the brazed joint of dissimilar Al 7075 and Al–25 Si alloy was 26.4 MPa. Th...
Saved in:
Main Authors: | Liu, Dashuang, Wei, Ping, Long, Weimin, Zhou, Wei |
---|---|
Other Authors: | School of Mechanical and Aerospace Engineering |
Format: | Article |
Language: | English |
Published: |
2023
|
Subjects: | |
Online Access: | https://hdl.handle.net/10356/165209 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Nanyang Technological University |
Language: | English |
Similar Items
-
Joining ferrite at a relatively low temperature using 43SnO-15ZnO-35P₂O₅-7SiO₂ phosphate glass braze
by: Guo, Wei, et al.
Published: (2022) -
Vacuum brazing of dissimilar aluminium alloys
by: Wong, Chun Long
Published: (2023) -
Strategy of incorporating Ni-based braze alloy in cold sprayed Inconel 718 coating
by: Sun, Wen, et al.
Published: (2021) -
Effect of Cu interlayer on the microstructure and strength for brazing of Tungsten/316L steel
by: Wang, Meng, et al.
Published: (2020) -
Numerical simulation of thermal processes in laser cladding of Al-50Si alloy on Al7075 surface
by: Kong, Meng
Published: (2022)