On the fatigue damage micromechanisms in Si-solution–strengthened spheroidal graphite cast iron

Graphite nodules in Spheroidal graphite cast iron (SGI) play a vital role in fatigue crack initiation and propagation. The graphite nodule growth morphology can go through transitions to form degenerated graphite nodules other than spheroidal graphite nodules in SGI microstructure. These graphite no...

Full description

Saved in:
Bibliographic Details
Main Authors: Sujakhu, Surendra, Castagne, Sylvie, Sakaguchi, M., Kasvayee, K. A., Ghassemali, E., Jarfors, A. E. W., Wang, W.
Other Authors: School of Mechanical and Aerospace Engineering
Format: Article
Language:English
Published: 2017
Subjects:
Online Access:https://hdl.handle.net/10356/85822
http://hdl.handle.net/10220/43880
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Nanyang Technological University
Language: English
id sg-ntu-dr.10356-85822
record_format dspace
spelling sg-ntu-dr.10356-858222023-03-04T17:15:54Z On the fatigue damage micromechanisms in Si-solution–strengthened spheroidal graphite cast iron Sujakhu, Surendra Castagne, Sylvie Sakaguchi, M. Kasvayee, K. A. Ghassemali, E. Jarfors, A. E. W. Wang, W. School of Mechanical and Aerospace Engineering Spheroidal graphite cast iron Damage micromechanisms Graphite nodules in Spheroidal graphite cast iron (SGI) play a vital role in fatigue crack initiation and propagation. The graphite nodule growth morphology can go through transitions to form degenerated graphite nodules other than spheroidal graphite nodules in SGI microstructure. These graphite nodules significantly influence damage micromechanisms on SGI and could act differently. Most of the damage mechanism studies on SGI were focused on the role of spheroidal graphite nodules on the stable crack propagation region. The roles of degenerated graphite nodules on SGI damage mechanisms were not frequently studied. In this work, fatigue crack initiation and propagation tests were conducted on EN-GJS-500-14 and observed under SEM to understand damage mechanisms of different graphite forms. Crack initiation tests showed dominant influence of degenerated graphite nodules where early cracks initiated in the microstructure. Most of the spheroidal graphite nodules were unaffected at the early crack initiation stage; some of them showed decohesion from the ferrite matrix and internal cracking. At the crack propagation region, graphite-ferrite matrix decohesion was the frequent damage mechanism observed with noticeable crack branching around graphite nodules and the crack passing through degenerated graphite nodules. Finally, graphite nodules after decohesion acted like voids which grew and coalesced to form microcracks eventually causing rapid fracture of the remaining section. MOE (Min. of Education, S’pore) Accepted version 2017-10-13T07:51:53Z 2019-12-06T16:10:49Z 2017-10-13T07:51:53Z 2019-12-06T16:10:49Z 2017 Journal Article Sujakhu, S., Castagne, S., Sakaguchi, M., Kasvayee, K. A., Ghassemali, E., Jarfors, A. E. W., et al. (2017). On the fatigue damage micromechanisms in Si-solution–strengthened spheroidal graphite cast iron. Fatigue & Fracture of Engineering Materials & Structures, in press. 8756-758X https://hdl.handle.net/10356/85822 http://hdl.handle.net/10220/43880 10.1111/ffe.12723 en Fatigue & Fracture of Engineering Materials & Structures © 2017 Wiley Publishing Ltd. This is the author created version of a work that has been peer reviewed and accepted for publication by Fatigue & Fracture of Engineering Materials & Structures, Wiley Publishing Ltd. It incorporates referee’s comments but changes resulting from the publishing process, such as copyediting, structural formatting, may not be reflected in this document. The published version is available at: [http://dx.doi.org/10.1111/ffe.12723]. 30 p. application/pdf
institution Nanyang Technological University
building NTU Library
continent Asia
country Singapore
Singapore
content_provider NTU Library
collection DR-NTU
language English
topic Spheroidal graphite cast iron
Damage micromechanisms
spellingShingle Spheroidal graphite cast iron
Damage micromechanisms
Sujakhu, Surendra
Castagne, Sylvie
Sakaguchi, M.
Kasvayee, K. A.
Ghassemali, E.
Jarfors, A. E. W.
Wang, W.
On the fatigue damage micromechanisms in Si-solution–strengthened spheroidal graphite cast iron
description Graphite nodules in Spheroidal graphite cast iron (SGI) play a vital role in fatigue crack initiation and propagation. The graphite nodule growth morphology can go through transitions to form degenerated graphite nodules other than spheroidal graphite nodules in SGI microstructure. These graphite nodules significantly influence damage micromechanisms on SGI and could act differently. Most of the damage mechanism studies on SGI were focused on the role of spheroidal graphite nodules on the stable crack propagation region. The roles of degenerated graphite nodules on SGI damage mechanisms were not frequently studied. In this work, fatigue crack initiation and propagation tests were conducted on EN-GJS-500-14 and observed under SEM to understand damage mechanisms of different graphite forms. Crack initiation tests showed dominant influence of degenerated graphite nodules where early cracks initiated in the microstructure. Most of the spheroidal graphite nodules were unaffected at the early crack initiation stage; some of them showed decohesion from the ferrite matrix and internal cracking. At the crack propagation region, graphite-ferrite matrix decohesion was the frequent damage mechanism observed with noticeable crack branching around graphite nodules and the crack passing through degenerated graphite nodules. Finally, graphite nodules after decohesion acted like voids which grew and coalesced to form microcracks eventually causing rapid fracture of the remaining section.
author2 School of Mechanical and Aerospace Engineering
author_facet School of Mechanical and Aerospace Engineering
Sujakhu, Surendra
Castagne, Sylvie
Sakaguchi, M.
Kasvayee, K. A.
Ghassemali, E.
Jarfors, A. E. W.
Wang, W.
format Article
author Sujakhu, Surendra
Castagne, Sylvie
Sakaguchi, M.
Kasvayee, K. A.
Ghassemali, E.
Jarfors, A. E. W.
Wang, W.
author_sort Sujakhu, Surendra
title On the fatigue damage micromechanisms in Si-solution–strengthened spheroidal graphite cast iron
title_short On the fatigue damage micromechanisms in Si-solution–strengthened spheroidal graphite cast iron
title_full On the fatigue damage micromechanisms in Si-solution–strengthened spheroidal graphite cast iron
title_fullStr On the fatigue damage micromechanisms in Si-solution–strengthened spheroidal graphite cast iron
title_full_unstemmed On the fatigue damage micromechanisms in Si-solution–strengthened spheroidal graphite cast iron
title_sort on the fatigue damage micromechanisms in si-solution–strengthened spheroidal graphite cast iron
publishDate 2017
url https://hdl.handle.net/10356/85822
http://hdl.handle.net/10220/43880
_version_ 1759857316380803072