On the fatigue damage micromechanisms in Si-solution–strengthened spheroidal graphite cast iron
Graphite nodules in Spheroidal graphite cast iron (SGI) play a vital role in fatigue crack initiation and propagation. The graphite nodule growth morphology can go through transitions to form degenerated graphite nodules other than spheroidal graphite nodules in SGI microstructure. These graphite no...
Saved in:
Main Authors: | Sujakhu, Surendra, Castagne, Sylvie, Sakaguchi, M., Kasvayee, K. A., Ghassemali, E., Jarfors, A. E. W., Wang, W. |
---|---|
Other Authors: | School of Mechanical and Aerospace Engineering |
Format: | Article |
Language: | English |
Published: |
2017
|
Subjects: | |
Online Access: | https://hdl.handle.net/10356/85822 http://hdl.handle.net/10220/43880 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Nanyang Technological University |
Language: | English |
Similar Items
-
Cast iron soil pipe and fitting
by: Sy, Tian Hui, et al.
Published: (1970) -
Cast iron soil pipe and fitting
by: Sy, Tian Hui, et al.
Published: (1970) -
Wear characteristics of sub-zero chilled cast iron
by: Seah, K.H.W., et al.
Published: (2014) -
Micromechanical characterization parameters for a new failure criterion for composite structures
by: Yudhanto, A., et al.
Published: (2014) -
Heat treatment characteristics of high chromium cast iron for abrasion wear resistance
by: Sudsakorn Inthidech
Published: (2006)