Spark plasma sintering of Sm2O3-doped aluminum nitride
The high sintering temperature required for aluminum nitride (AlN) at typically 1800 °C, is an impediment to its development as an engineering material. Spark plasma sintering (SPS) of AlN is carried out with samarium oxide (Sm2O3) as sintering additive at a sintering temperature as low as 1500–1600...
Saved in:
Main Authors: | Khor, Khiam Aik, Yu, L. G., Murakoshi, Y. |
---|---|
Other Authors: | School of Mechanical and Aerospace Engineering |
Format: | Article |
Language: | English |
Published: |
2012
|
Subjects: | |
Online Access: | https://hdl.handle.net/10356/95602 http://hdl.handle.net/10220/8236 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Nanyang Technological University |
Language: | English |
Similar Items
-
Spark plasma sintering of aluminum nitride
by: Tan, Mui Ting.
Published: (2008) -
Spark-plasma-sintering (SPS) of nanostructured and submicron titanium oxide powders
by: Angerer, P., et al.
Published: (2012) -
Spark-plasma-sintering (SPS) of nanostructured titanium carbonitride powders
by: Angerer, P., et al.
Published: (2012) -
Boride layer growth kinetics during boriding of molybdenum by the Spark Plasma Sintering (SPS) technology
by: Yu, L. G., et al.
Published: (2012) -
Nanostructural characteristics, mechanical properties, and osteoblast response of spark plasma sintered hydroxyapatite
by: Li, H., et al.
Published: (2012)