Microstructure and erosion-corrosion behaviour of as-cast high chromium white irons containing molybdenum in aqueous sulfuric-acid slurry

Microstructure and erosion-corrosion behaviour of as-cast high chromium white irons containing molybdenum in aqueous sulfuric-acid slurry was studied. The experimental irons contained 28 wt.%Cr with a Cr:C ratio of about 10 and up to 10 wt.%Mo. The irons with up to 6 wt.%Mo are hypoeutectic, whereas...

Full description

Saved in:
Bibliographic Details
Main Authors: S. Imurai, Ch Thanachayanont, J. T.H. Pearce, T. Chairuangsri
Format: Journal
Published: 2018
Subjects: