Isothermal phase transformation sequence in Fe-22wt%Cr-3.2wt%Mo-6.2wt%Ni-0.037wt%C cast duplex stainless steel

Isothermal phase transformation behaviour in a Fe-22wt%Cr-3.2wt%Mo-6.2wt% Ni-0.037wt%C cast duplex stainless steel has been studied. The steel was solution heat-treated at 1175°C for 1 hour and isothermally heat-treated in the temperature range of 500-1,000°C for 8 to 32 hours, followed by water que...