Fracture toughness assessment of a solder joint using double cantilever beam specimens

Conventional assessment of solder joint reliability uses either ball shear test or solder ball pull test. The test results are reported in terms of materials strength in either shear or tensile mode, and the strength values are size-dependent. Therefore these test results are largely useful only for...

Full description

Saved in:
Bibliographic Details
Main Authors: Lee, Adeline Puay Chen, Lim, Zan Xuan, Yantara, Natalia, Loo, Shane Zhi Yuan, Tee, Tong Yan, Tan, Cher Ming, Chen, Zhong
Other Authors: School of Electrical and Electronic Engineering
Format: Conference or Workshop Item
Language:English
Published: 2010
Subjects:
Online Access:https://hdl.handle.net/10356/91518
http://hdl.handle.net/10220/6384
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Nanyang Technological University
Language: English
id sg-ntu-dr.10356-91518
record_format dspace
spelling sg-ntu-dr.10356-915182020-03-07T13:24:46Z Fracture toughness assessment of a solder joint using double cantilever beam specimens Lee, Adeline Puay Chen Lim, Zan Xuan Yantara, Natalia Loo, Shane Zhi Yuan Tee, Tong Yan Tan, Cher Ming Chen, Zhong School of Electrical and Electronic Engineering Electronics Packaging Technology Conference (10th : 2008 : Singapore) Amkor Technology Singapore Pte Ltd DRNTU::Engineering::Electrical and electronic engineering::Electronic apparatus and materials DRNTU::Engineering::Materials Conventional assessment of solder joint reliability uses either ball shear test or solder ball pull test. The test results are reported in terms of materials strength in either shear or tensile mode, and the strength values are size-dependent. Therefore these test results are largely useful only for qualitative comparison and qualification of the products. In the current effort, we aim at developing an assessment scheme for solder joint interface fracture toughness. The obtained results, in terms of critical energy release rate, predict the joint failure based on the principle of fracture mechanics. The results can be used as a materials property in the reliability design of various types of solder-ball joined packages. Double cantilever beam (DCB) specimens made of 99.9 wt% copper were selected in the current work. Eutectic Sn-37Pb solder was used to join two pieces of the copper plates with controlled solder thickness. The test record showed steady propagation of the crack along the solder/copper interface, which verifies the viability of such a testing scheme. Interface fracture toughness for as-joined, extensively-reflowed and thermally aged samples has been measured. Both the reflow treatment and the thermal aging lead to degradation of solder joint fracture resistance. To understand the degradation, fractographic analysis by scanning electron microscopy (SEM) has been carried out from both top and cross-sectional views of the fractured surfaces. Published version 2010-08-31T07:07:04Z 2019-12-06T18:07:08Z 2010-08-31T07:07:04Z 2019-12-06T18:07:08Z 2008 2008 Conference Paper Lee, A. P. C., Lim, Z. X., Yantara, N., Loo, S. Z. Y., Tee, T. Y., Tan, C. M., et al. (2008). Fracture toughness assessment of a solder joint using double cantilever beam specimens. In proceedings of the 10th Electronics Packaging Technology Conference: Singapore, (pp.1066-1073). https://hdl.handle.net/10356/91518 http://hdl.handle.net/10220/6384 10.1109/EPTC.2008.4763571 en © 2008 IEEE. Personal use of this material is permitted. However, permission to reprint/republish this material for advertising or promotional purposes or for creating new collective works for resale or redistribution to servers or lists, or to reuse any copyrighted component of this work in other works must be obtained from the IEEE. This material is presented to ensure timely dissemination of scholarly and technical work. Copyright and all rights therein are retained by authors or by other copyright holders. All persons copying this information are expected to adhere to the terms and constraints invoked by each author's copyright. In most cases, these works may not be reposted without the explicit permission of the copyright holder. http://www.ieee.org/portal/site This material is presented to ensure timely dissemination of scholarly and technical work. Copyright and all rights therein are retained by authors or by other copyright holders. All persons copying this information are expected to adhere to the terms and constraints invoked by each author's copyright. In most cases, these works may not be reposted without the explicit permission of the copyright holder. 8 p. application/pdf
institution Nanyang Technological University
building NTU Library
country Singapore
collection DR-NTU
language English
topic DRNTU::Engineering::Electrical and electronic engineering::Electronic apparatus and materials
DRNTU::Engineering::Materials
spellingShingle DRNTU::Engineering::Electrical and electronic engineering::Electronic apparatus and materials
DRNTU::Engineering::Materials
Lee, Adeline Puay Chen
Lim, Zan Xuan
Yantara, Natalia
Loo, Shane Zhi Yuan
Tee, Tong Yan
Tan, Cher Ming
Chen, Zhong
Fracture toughness assessment of a solder joint using double cantilever beam specimens
description Conventional assessment of solder joint reliability uses either ball shear test or solder ball pull test. The test results are reported in terms of materials strength in either shear or tensile mode, and the strength values are size-dependent. Therefore these test results are largely useful only for qualitative comparison and qualification of the products. In the current effort, we aim at developing an assessment scheme for solder joint interface fracture toughness. The obtained results, in terms of critical energy release rate, predict the joint failure based on the principle of fracture mechanics. The results can be used as a materials property in the reliability design of various types of solder-ball joined packages. Double cantilever beam (DCB) specimens made of 99.9 wt% copper were selected in the current work. Eutectic Sn-37Pb solder was used to join two pieces of the copper plates with controlled solder thickness. The test record showed steady propagation of the crack along the solder/copper interface, which verifies the viability of such a testing scheme. Interface fracture toughness for as-joined, extensively-reflowed and thermally aged samples has been measured. Both the reflow treatment and the thermal aging lead to degradation of solder joint fracture resistance. To understand the degradation, fractographic analysis by scanning electron microscopy (SEM) has been carried out from both top and cross-sectional views of the fractured surfaces.
author2 School of Electrical and Electronic Engineering
author_facet School of Electrical and Electronic Engineering
Lee, Adeline Puay Chen
Lim, Zan Xuan
Yantara, Natalia
Loo, Shane Zhi Yuan
Tee, Tong Yan
Tan, Cher Ming
Chen, Zhong
format Conference or Workshop Item
author Lee, Adeline Puay Chen
Lim, Zan Xuan
Yantara, Natalia
Loo, Shane Zhi Yuan
Tee, Tong Yan
Tan, Cher Ming
Chen, Zhong
author_sort Lee, Adeline Puay Chen
title Fracture toughness assessment of a solder joint using double cantilever beam specimens
title_short Fracture toughness assessment of a solder joint using double cantilever beam specimens
title_full Fracture toughness assessment of a solder joint using double cantilever beam specimens
title_fullStr Fracture toughness assessment of a solder joint using double cantilever beam specimens
title_full_unstemmed Fracture toughness assessment of a solder joint using double cantilever beam specimens
title_sort fracture toughness assessment of a solder joint using double cantilever beam specimens
publishDate 2010
url https://hdl.handle.net/10356/91518
http://hdl.handle.net/10220/6384
_version_ 1681047859153076224