Formation of titanium nitride on γ-TiAl alloys by direct metal-gas reaction
Two alloys, Ti-47Al-2Nb-2Cr (MJ12) and Ti-47Al-2Nb-2Mn + 0.8TiB2(MJ47), were nitrided in purified ammonia for 3.6 × 103-3.6 × 104s (1-10 h) at a temperature range of 800-1,000 °C. The nitridation process can successfully improve alloy hardness which increased with an increase of the nitridation temp...
Saved in:
Main Authors: | Kittichai Sopunna, Titipun Thongtem, Michael McNallan, Somchai Thongtem |
---|---|
Format: | Journal |
Published: |
2018
|
Subjects: | |
Online Access: | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=33747088193&origin=inward http://cmuir.cmu.ac.th/jspui/handle/6653943832/61745 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Institution: | Chiang Mai University |
Similar Items
-
Surface modification of the γ-TiAl alloys by the nitridation
by: Sopunna K., et al.
Published: (2014) -
Nitridation of γ-TiAl alloys by direct metal-gas reaction at 1000-1300 K
by: Somchai Thongtem, et al.
Published: (2018) -
Nitridation of γ-TiAl alloys by direct metal-gas reaction at 1000-1300 K
by: Thongtem S., et al.
Published: (2014) -
Effect of nitridation and carburization of γ-TiAl alloys on wear resistance
by: Boonruang C., et al.
Published: (2014) -
Surface modification of γ-TiAl alloys by acetylene plasma deposition
by: Suparut Narksitipan, et al.
Published: (2018)