Reduction of threading dislocation density in Ge/Si using a heavily As-doped Ge seed layer

High quality germanium(Ge)epitaxialfilm is grown directly on silicon (001) substrate with 6° off-cut using a heavily arsenic (As) dopedGe seed layer. The growth steps consists of (i) growth of a heavily As-doped Ge seed layer at low temperature (LT, at 400 °C), (ii) Gegrowth with As gradually reduce...

Full description

Saved in:
Bibliographic Details
Main Authors: Lee, Kwang Hong, Bao, Shuyu, Wang, Bing, Wang, Cong, Yoon, Soon Fatt, Michel, Jurgen, Fitzgerald, Eugene A., Tan, Chuan Seng
Other Authors: School of Electrical and Electronic Engineering
Format: Article
Language:English
Published: 2016
Subjects:
Online Access:https://hdl.handle.net/10356/84177
http://hdl.handle.net/10220/41651
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Nanyang Technological University
Language: English
id sg-ntu-dr.10356-84177
record_format dspace
spelling sg-ntu-dr.10356-841772020-03-07T14:00:34Z Reduction of threading dislocation density in Ge/Si using a heavily As-doped Ge seed layer Lee, Kwang Hong Bao, Shuyu Wang, Bing Wang, Cong Yoon, Soon Fatt Michel, Jurgen Fitzgerald, Eugene A. Tan, Chuan Seng School of Electrical and Electronic Engineering Germanium Elemental semiconductors High quality germanium(Ge)epitaxialfilm is grown directly on silicon (001) substrate with 6° off-cut using a heavily arsenic (As) dopedGe seed layer. The growth steps consists of (i) growth of a heavily As-doped Ge seed layer at low temperature (LT, at 400 °C), (ii) Gegrowth with As gradually reduced to zero at high temperature (HT, at 650 °C), (iii) pure Gegrowth at HT. This is followed by thermal cyclic annealing in hydrogen at temperature ranging from 600 to 850 °C. Analytical characterization have shown that the Geepitaxialfilm with a thickness of ∼1.5 µm experiences thermally induced tensile strain of 0.20% with a treading dislocation density (TDD) of mid 106/cm2 which is one order of magnitude lower than the control group without As doping and surface roughness of 0.37 nm. The reduction in TDD is due to the enhancement in velocity of dislocations in an As-doped Gefilm. NRF (Natl Research Foundation, S’pore) Published version 2016-11-29T08:48:38Z 2019-12-06T15:39:55Z 2016-11-29T08:48:38Z 2019-12-06T15:39:55Z 2016 Journal Article Lee, K. H., Bao, S., Wang, B., Wang, C., Yoon, S. F., Michel, J., et al. (2016). Reduction of threading dislocation density in Ge/Si using a heavily As-doped Ge seed layer. AIP Advances, 6(2), 025028-. 2158-3226 https://hdl.handle.net/10356/84177 http://hdl.handle.net/10220/41651 10.1063/1.4943218 en AIP Advances © 2016 The Author(s) (published by American Institute of Physics). All article content, except where otherwise noted, is licensed under a Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/). 8 p. application/pdf
institution Nanyang Technological University
building NTU Library
country Singapore
collection DR-NTU
language English
topic Germanium
Elemental semiconductors
spellingShingle Germanium
Elemental semiconductors
Lee, Kwang Hong
Bao, Shuyu
Wang, Bing
Wang, Cong
Yoon, Soon Fatt
Michel, Jurgen
Fitzgerald, Eugene A.
Tan, Chuan Seng
Reduction of threading dislocation density in Ge/Si using a heavily As-doped Ge seed layer
description High quality germanium(Ge)epitaxialfilm is grown directly on silicon (001) substrate with 6° off-cut using a heavily arsenic (As) dopedGe seed layer. The growth steps consists of (i) growth of a heavily As-doped Ge seed layer at low temperature (LT, at 400 °C), (ii) Gegrowth with As gradually reduced to zero at high temperature (HT, at 650 °C), (iii) pure Gegrowth at HT. This is followed by thermal cyclic annealing in hydrogen at temperature ranging from 600 to 850 °C. Analytical characterization have shown that the Geepitaxialfilm with a thickness of ∼1.5 µm experiences thermally induced tensile strain of 0.20% with a treading dislocation density (TDD) of mid 106/cm2 which is one order of magnitude lower than the control group without As doping and surface roughness of 0.37 nm. The reduction in TDD is due to the enhancement in velocity of dislocations in an As-doped Gefilm.
author2 School of Electrical and Electronic Engineering
author_facet School of Electrical and Electronic Engineering
Lee, Kwang Hong
Bao, Shuyu
Wang, Bing
Wang, Cong
Yoon, Soon Fatt
Michel, Jurgen
Fitzgerald, Eugene A.
Tan, Chuan Seng
format Article
author Lee, Kwang Hong
Bao, Shuyu
Wang, Bing
Wang, Cong
Yoon, Soon Fatt
Michel, Jurgen
Fitzgerald, Eugene A.
Tan, Chuan Seng
author_sort Lee, Kwang Hong
title Reduction of threading dislocation density in Ge/Si using a heavily As-doped Ge seed layer
title_short Reduction of threading dislocation density in Ge/Si using a heavily As-doped Ge seed layer
title_full Reduction of threading dislocation density in Ge/Si using a heavily As-doped Ge seed layer
title_fullStr Reduction of threading dislocation density in Ge/Si using a heavily As-doped Ge seed layer
title_full_unstemmed Reduction of threading dislocation density in Ge/Si using a heavily As-doped Ge seed layer
title_sort reduction of threading dislocation density in ge/si using a heavily as-doped ge seed layer
publishDate 2016
url https://hdl.handle.net/10356/84177
http://hdl.handle.net/10220/41651
_version_ 1681040067325329408