Reactive blending of thermoplastic starch, epoxidized natural rubber and chitosan

© 2016 Thermoplastic starch (TPS) was prepared by melt blending cassava starch and glycerol (70/30) at 140 °C. Chitosan (CTS) was incorporated during TPS preparation. The TPS/CTS sample was melt blended with epoxidized natural rubber (ENR) at 140 °C. In the TPS/ENR/CTS blend, adding CTS and ENR impr...

Full description

Saved in:
Bibliographic Details
Main Authors: Jantanasakulwong K., Leksawasdi N., Seesuriyachan P., Wongsuriyasak S., Techapun C., Ougizawa T.
Format: Journal
Published: 2017
Online Access:https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84988697878&origin=inward
http://cmuir.cmu.ac.th/jspui/handle/6653943832/41378
Tags: Add Tag
No Tags, Be the first to tag this record!
Institution: Chiang Mai University
Description
Summary:© 2016 Thermoplastic starch (TPS) was prepared by melt blending cassava starch and glycerol (70/30) at 140 °C. Chitosan (CTS) was incorporated during TPS preparation. The TPS/CTS sample was melt blended with epoxidized natural rubber (ENR) at 140 °C. In the TPS/ENR/CTS blend, adding CTS and ENR improved the tensile strength and elongation at break, respectively. Morphology of the TPS/ENR blend showed the dispersion of large-sized ENR particles in the TPS matrix. Adding CTS reduced the size of the ENR particles. Incorporating CTS also enhanced the melt viscosity of the blend, which suggested a reaction between CTS and ENR. FTIR confirmed that the amino groups of CTS reacted with the epoxy groups of ENR. This reaction between the CTS amino groups with the ENR epoxy groups improved the mechanical properties of the TPS/ENR/CTS blend.