Reactive blending of thermoplastic starch, epoxidized natural rubber and chitosan
© 2016 Thermoplastic starch (TPS) was prepared by melt blending cassava starch and glycerol (70/30) at 140 °C. Chitosan (CTS) was incorporated during TPS preparation. The TPS/CTS sample was melt blended with epoxidized natural rubber (ENR) at 140 °C. In the TPS/ENR/CTS blend, adding CTS and ENR impr...